MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Glass Reinforced, Impact Modified

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.960 - 1.44 g/cc0.0347 - 0.0520 lb/in³Average value: 1.11 g/cc Grade Count:83
Filler Content 10.0 - 50.0 %10.0 - 50.0 %Average value: 26.9 % Grade Count:27
Water Absorption 0.0100 - 0.0600 %0.0100 - 0.0600 %Average value: 0.0277 % Grade Count:13
Linear Mold Shrinkage 0.00100 - 0.0226 cm/cm0.00100 - 0.0226 in/inAverage value: 0.00513 cm/cm Grade Count:40
Linear Mold Shrinkage, Transverse 0.00300 - 0.0210 cm/cm0.00300 - 0.0210 in/inAverage value: 0.0124 cm/cm Grade Count:6
Melt Flow 0.900 - 22.7 g/10 min0.900 - 22.7 g/10 minAverage value: 8.09 g/10 min Grade Count:56
Ash 27.0 - 27.0 %
@Temperature 625 - 625 °C
27.0 - 27.0 %
@Temperature 1160 - 1160 °F
Average value: 27.0 % Grade Count:1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 83.0 - 11583.0 - 115Average value: 96.9 Grade Count:17
Hardness, Shore D 52.0 - 80.052.0 - 80.0Average value: 62.2 Grade Count:6
Tensile Strength, Ultimate 20.0 - 120 MPa2900 - 17400 psiAverage value: 61.1 MPa Grade Count:41
Tensile Strength, Yield 31.0 - 95.0 MPa4500 - 13800 psiAverage value: 50.7 MPa Grade Count:24
Elongation at Break 2.00 - 36.0 %2.00 - 36.0 %Average value: 7.63 % Grade Count:47
Elongation at Yield 0.600 - 4.50 %0.600 - 4.50 %Average value: 2.53 % Grade Count:4
Modulus of Elasticity 1.50 - 9.50 GPa218 - 1380 ksiAverage value: 4.77 GPa Grade Count:26
Flexural Yield Strength 4.48 - 155 MPa650 - 22500 psiAverage value: 85.3 MPa Grade Count:40
Flexural Modulus 1.50 - 9.50 GPa218 - 1380 ksiAverage value: 3.70 GPa Grade Count:82
Izod Impact, Notched 0.518 - 2.14 J/cm0.970 - 4.00 ft-lb/inAverage value: 1.22 J/cm Grade Count:29
 1.30 - 1.30 J/cm
@Temperature -40.0 - -40.0 °C
2.44 - 2.44 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 1.30 J/cm Grade Count:2
Izod Impact, Unnotched 2.14 - 8.01 J/cm4.00 - 15.0 ft-lb/inAverage value: 5.04 J/cm Grade Count:20
 4.80 - 4.80 J/cm
@Temperature -40.0 - -40.0 °C
8.99 - 8.99 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 4.80 J/cm Grade Count:2
Izod Impact, Notched (ISO) 3.00 - 37.0 kJ/m²1.43 - 17.6 ft-lb/in²Average value: 20.2 kJ/m² Grade Count:23
 5.00 - 20.0 kJ/m²
@Temperature -40.0 - -30.0 °C
2.38 - 9.52 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 7.92 kJ/m² Grade Count:13
Izod Impact, Unnotched (ISO) 40.0 - 70.0 kJ/m²19.0 - 33.3 ft-lb/in²Average value: 47.0 kJ/m² Grade Count:5
Charpy Impact Unnotched 1.60 - 7.50 J/cm²7.61 - 35.7 ft-lb/in²Average value: 4.70 J/cm² Grade Count:9
 1.00 - 6.50 J/cm²
@Temperature -40.0 - -20.0 °C
4.76 - 30.9 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 3.82 J/cm² Grade Count:6
Charpy Impact, Notched 0.200 - 4.50 J/cm²0.952 - 21.4 ft-lb/in²Average value: 2.47 J/cm² Grade Count:31
 0.100 - 2.00 J/cm²
@Temperature -40.0 - 0.000 °C
0.476 - 9.52 ft-lb/in²
@Temperature -40.0 - 32.0 °F
Average value: 0.824 J/cm² Grade Count:30
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 - 1.00e+16 ohm-cm1.00e+12 - 1.00e+16 ohm-cmAverage value: 6.45e+15 ohm-cm Grade Count:16
Surface Resistance 1.00e+12 - 1.00e+14 ohm1.00e+12 - 1.00e+14 ohmAverage value: 6.70e+13 ohm Grade Count:3
 
Thermal PropertiesMetricEnglishComments
Melting Point 145 - 168 °C293 - 334 °FAverage value: 159 °C Grade Count:9
Deflection Temperature at 0.46 MPa (66 psi) 125 - 166 °C257 - 331 °FAverage value: 143 °C Grade Count:52
Deflection Temperature at 1.8 MPa (264 psi) 67.0 - 160 °C153 - 320 °FAverage value: 128 °C Grade Count:47
Vicat Softening Point 95.0 - 165 °C203 - 329 °FAverage value: 141 °C Grade Count:14
Flammability, UL94 HB - V-0HB - V-0Grade Count:18
Glow Wire Test 650 - 960 °C1200 - 1760 °FAverage value: 857 °C Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 250 °C374 - 482 °FAverage value: 211 °C Grade Count:24
Melt Temperature 170 - 250 °C338 - 482 °FAverage value: 228 °C Grade Count:10
Mold Temperature 32.2 - 90.0 °C90.0 - 194 °FAverage value: 61.6 °C Grade Count:29
Drying Temperature 80.0 - 100 °C176 - 212 °FAverage value: 96.3 °C Grade Count:12
Injection Pressure 40.0 - 130 MPa5800 - 18900 psiAverage value: 89.6 MPa Grade Count:27

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Extrusion Grade
Overview of materials for Polypropylene with 40% Glass Fiber Filler
Overview of materials for Polypropylene, Molded
Overview of materials for Polypropylene with 50% Glass Fiber Filler
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded

O4719 / 78384

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.