MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman AP005 Copolyester  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Applications:
  • Automotive components
  • Breathable films
  • Electrical/electronic components
  • Film Modification
  • Flexible hinges
  • Hose mandrel
  • Industrial components
  • Industrial hoses/belts
  • Office furniture
  • Packaging
  • Polymer modification
  • Profiles
  • Rubber and plastic modification
  • Sporting goods
  • Thermoplastic elastomer compounds
  • Tubing

Key Attributes:

  • Environmentally preferred, non-halogenated material
  • Excellent chemical and oil resistance
  • Excellent compatibility with a wide range of polymers
  • Excellent processability
  • Exceptional heat resistance and high temperature dimensional stability
  • High energy absorption
  • High flexibility without plasticizers
  • Melt bondable to a variety of substrates, including PVC
  • Outstanding toughness and puncture resistance
  • Solvent bondable

Product Description: Eastman AP005 is a tough, clear, durable copolyester ether that combines the strength of plastics, the flexibility of elastomers, and the processability of thermoplastics. Eastman AP005 can be used in injection molding and film or tubing extrusion applications or in any application that demands strength, durability, chemical resistance, and puncture resistance in harsh environments. This copolyester combines toughness, clarity, high temperature resistance and flexibility without the addition of plasticizers. Eastman AP005 is considered environmentally preferred because of its non-halogenated material composition. Its broad compatibility with other polymers such as styrenic block copolymers makes it an excellent choice for both alloys and as additives/modifiers to improve performance properties.

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D792
Water Absorption 0.35 %
@Time 86400 sec
0.35 %
@Time 24.0 hour
Immersion; ASTM D570
Water Vapor Transmission 132 g/m²/day8.50 g/100 in²/dayASTM F372
Oxygen Transmission Rate 841 cc/m²/day
@Pressure 0.101 MPa,
Temperature 30.0 °C
54.2 cc/100 in²/day
@Pressure 14.7 psi,
Temperature 86.0 °F
ASTM D1434
Viscosity Measurement 1.051.05Inherent; EMN-A-AC-G-V-1
Thickness 130 microns5.12 mil
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595ASTM D2240
Hardness, Shore D 5555ASTM D2240
Tensile Strength at Break 20.0 MPa2900 psiASTM D638
Film Tensile Strength at Yield, MD 13.7 MPa1990 psiASTM D882
Film Tensile Strength at Yield, TD 13.5 MPa1960 psiASTM D882
Tensile Strength, Yield 14.0 MPa2030 psiASTM D638
Film Elongation at Break, MD 550 %550 %ASTM D882
Film Elongation at Break, TD 550 %550 %ASTM D882
Film Elongation at Yield, MD 26 %26 %ASTM D882
Film Elongation at Yield, TD 26 %26 %ASTM D882
Elongation at Break 300 %300 %ASTM D638
Elongation at Yield 30 %30 %ASTM D638
Tensile Modulus 0.170 GPa24.7 ksiASTM D638
Flexural Modulus 0.150 GPa21.8 ksiASTM D790
Izod Impact, Notched 0.500 J/cm
@Temperature -40.0 °C
0.937 ft-lb/in
@Temperature -40.0 °F
ASTM D256
Coefficient of Friction >= 1.0>= 1.0ASTM D1894
Tear Strength, Total 370 N83.2 lb (f)ASTM D1004
Film Tensile Strength at Break, MD 23.7 MPa3440 psiASTM D882
Film Tensile Strength at Break, TD 22.6 MPa3280 psiASTM D882
Tangent Modulus 179 MPa26000 psiT.D.; ASTM D882
 185 MPa26800 psiM.D.; ASTM D882
Torsional Stiffness  240 MPa
@Temperature -28.0 °C
34800 psi
@Temperature -18.4 °F
ASTM D1043
 930 MPa
@Temperature <=-70.0 °C
135000 psi
@Temperature <=-94.0 °F
ASTM D1043
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 27.0 J/g11.6 BTU/lbASTM E793
CTE, linear 150 µm/m-°C83.3 µin/in-°FASTM D696
Specific Heat Capacity  1.60 J/g-°C
@Temperature 25.0 °C
0.382 BTU/lb-°F
@Temperature 77.0 °F
solid; DSC
 1.80 J/g-°C
@Temperature 100 °C
0.430 BTU/lb-°F
@Temperature 212 °F
solid; DSC
 2.00 J/g-°C
@Temperature 150 °C
0.478 BTU/lb-°F
@Temperature 302 °F
solid; DSC
 2.30 J/g-°C
@Temperature 175 °C
0.550 BTU/lb-°F
@Temperature 347 °F
solid; DSC
 2.30 J/g-°C
@Temperature 225 °C
0.550 BTU/lb-°F
@Temperature 437 °F
melt; DSC
 3.10 J/g-°C
@Temperature 200 °C
0.741 BTU/lb-°F
@Temperature 392 °F
transition; DSC
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°FASTM C177
Melting Point 207 °C405 °FCrystalline Peak; ASTM D3418
Crystallization Temperature 140 °C284 °FDSC
Vicat Softening Point 170 °C
@Load 1.00 kg
338 °F
@Load 2.20 lb
ASTM D1525
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D746
Glass Transition Temp, Tg -3.00 °C26.6 °FDSC
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.51
@Wavelength 589.3 nm
1.51
@Wavelength 589.3 nm
nD; ASTM D542
Haze 1.0 %1.0 %for Film; ASTM D1003
Gloss 80 %80 %for Film, 45°; ASTM D2457
Transmission, Visible  90 %
@Thickness 0.130 mm
90 %
@Thickness 0.00512 in
Regular, Film; ASTM D1003
 93 %
@Thickness 0.130 mm
93 %
@Thickness 0.00512 in
Total, Film; ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman AP006 Copolyester
Eastman AP007 Copolyester
Eastman Eastar DN001HF Copolyester
Eastman Tritan™ FX100 Copolyester
Eastman Eastar CN015 Copolyester, High Flow Grade with Mold Release

PE8812 / 129657

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.