MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Medium-Silicon Ductile Iron, heat-resistant ductile iron
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; Ductile Iron

Material Notes: Ferrite matrix structure as cast.

Key Words: Heat-resistant ductile iron medium-silicon ductile iron, ferritic
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.11 g/cc0.257 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 140 - 300140 - 300
Tensile Strength 415 - 690 MPa60200 - 100000 psi
Tensile Strength, Yield 310 - 520 MPa45000 - 75400 psi
Elongation at Break 0.20 %0.20 %
Charpy Impact, Unnotched 7.00 - 155 J
@Diameter 10.0 mm
5.16 - 114 ft-lb
@Diameter 0.394 in
Standard Unnotched Charpy test
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000580 - 0.0000870 ohm-cm0.0000580 - 0.0000870 ohm-cmaverage
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.8 - 13.5 µm/m-°C
@Temperature 21.0 °C
6.00 - 7.50 µin/in-°F
@Temperature 69.8 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 2.8 - 3.8 %2.8 - 3.8 %
Iron, Fe 90 %90 %
Manganese, Mn 0.20 - 0.60 %0.20 - 0.60 %
Nickel, Ni <= 1.5 %<= 1.5 %
Phosphorus, P <= 0.080 %<= 0.080 %
Silicon, Si 2.5 - 6.0 %2.5 - 6.0 %
Sulfur, S <= 0.12 %<= 0.12 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
High-Nickel Ductile Iron, corrosion resistant
Gray Cast Iron, ASTM A 48 Class 40
High-Nickel Ductile Iron, heat-resistant ductile iron, 20% Ni
Ductile Iron grade 60-40-18
Overview of materials for Ductile Iron

MAFEB3 / 10242

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.