MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trelleborg AEM Eccospheres® IG-101 Sodium Borosilicate Glass Microspheres
Categories: Ceramic; Glass; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnification reveals them to be near perfect spheres.

    Properties
  • High temperature resistance
  • Good density/strength ratios
  • Clean surface chemistry
  • Narrow particle size distribution
  • Low thermal conductivity
  • Low dielectric constant
  • Low dissipation factor

Specifically developed for industrial applications the IG series of Eccospheres® glass microspheres are manufactured to the same high standards as other series. This range does not undergo final washing or floating processes.

All information provided by Trelleborg Emerson & Cuming

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Pellet Density 0.330 - 0.370 g/cc0.0119 - 0.0134 lb/in³ASTM D2840
Particle Size 55 µm55 µmTEC QSD
pH 6.5 - 9.06.5 - 9.0ASTM D4876
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity  62.0 GPa
@Temperature 25.0 °C
8990 ksi
@Temperature 77.0 °F
 62.0 GPa
@Temperature 25.0 °C
8990 ksi
@Temperature 77.0 °F
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 1.36 - 1.63
@Frequency 1e+8 Hz
1.36 - 1.63
@Frequency 1e+8 Hz
ASTM D150
Dissipation Factor 0.00050
@Frequency 1e+6 - 8.60e+9 Hz
0.00050
@Frequency 1e+6 - 8.60e+9 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0730 - 0.125 W/m-K0.507 - 0.868 BTU-in/hr-ft²-°F
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.448
@Wavelength 1500 nm
1.448
@Wavelength 1500 nm
 1.458
@Wavelength 589.3 nm
1.458
@Wavelength 589.3 nm
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 1.0 %<= 1.0 %TED QSD
 
Descriptive Properties
Floatation (% bulk volume)96TEC QSD
Isostatic Collapse Pressure, Min. 80% Survival (psi)1500ASTM D3102
Packing Factor (min)62

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg AEM Eccospheres® SI-250 Sodium Borosilicate Glass Microspheres
3M K37 Glass Bubbles
3M S38HS Glass Bubbles
3M S38 Glass Bubbles
Celanese 50000445 Methyl Isobutyl Carbinol (MIBC)

PTRELL180 / 83938

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.