Product Description: ExxonMobil™ LD 07024 Series case wrap film resins combine good processability with excellent strength and good film optics forbundlingapplications requiring proper shrink performance, toughness and burn-through resistance and clarity Availability: Latin America, North America Additive: - Antiblock: 4000 ppm
- Slip: No
- Thermal Stabilizer: No
Applications:- Blend Partner
- Co-Extrusion Films
- Collation Shrink
- Construction Film
- Form Fill and Seal Packaging
- Freezer Film
- Lamination Film
- Medium Duty Shrink Film
- Pallet Shrink Film
Information provided by ExxonMobil |