MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex APEX® 1009 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade; PVC, Wire and Cable Grade

Material Notes: Notes: 60°C General Purpose; RoHS Compliant

Uses: Connectors; Grommets; Plugs; Strain Reliefs

Forms: Pellets

Processing Method: Injection Molding

Agency Ratings: UL QMFZ2 .E54709

Wire Types: Molded Components

Additional Information:

Temperature Rating: 60°C

Recognized Component, CSA C22.2 No. 0.6, CSA Flammability Classification: 0.6HB at 0.88mm

Information Provided by Teknor Apex

Key Words: PVC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.37 g/cc1.37 g/ccASTM D792
Linear Mold Shrinkage 0.010 - 0.012 cm/cm0.010 - 0.012 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 868610 seconds; ASTM D2240
Tensile Strength at Break 11.7 MPa1700 psiASTM D638
Elongation at Break 260 %260 %ASTM D638
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index >= 600 V
@Thickness 3.00 mm
>= 600 V
@Thickness 0.118 in
UL 746
Hot Wire Ignition, HWI 60 - 120 sec
@Thickness 3.00 mm
60 - 120 sec
@Thickness 0.118 in
UL 746
High Amp Arc Ignition, HAI 60 - 120 arcs
@Thickness 3.00 mm
60 - 120 arcs
@Thickness 0.118 in
UL 746
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 60.0 °C140 °FContinuous Use; ASTM D794
Brittleness Temperature -25.0 °C-13.0 °FASTM D746
UL RTI, Electrical  90.0 °C
@Thickness 0.889 mm
194 °F
@Thickness 0.0350 in
UL 746
 90.0 °C
@Thickness 1.40 mm
194 °F
@Thickness 0.0551 in
UL 746
 90.0 °C
@Thickness 3.00 mm
194 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  80.0 °C
@Thickness 0.889 mm
176 °F
@Thickness 0.0350 in
UL 746
 80.0 °C
@Thickness 1.40 mm
176 °F
@Thickness 0.0551 in
UL 746
 90.0 °C
@Thickness 3.00 mm
194 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  HB
@Thickness 1.20 mm
HB
@Thickness 0.0472 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Oxygen Index 24 %24 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 °C360 °FProcessing Temperature
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex APEX® 02-A0033A-65 NT1 Polyvinyl Chloride, Flexible
Teknor Apex APEX® 1002 Polyvinyl Chloride, Flexible
Teknor Apex APEX® 1519-39 Polyvinyl Chloride, Flexible
Teknor Apex APEX® 1008 Polyvinyl Chloride, Flexible
Teknor Apex APEX® 1007 Polyvinyl Chloride, Flexible

PTEKNO551 / 128729

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.