MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ferro Aluminum Oxide P87
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Manufactured at the Diamonite Plant in Shreve, Ohio. Data provided by the manufacturer, Ferro Corporation.

Key Words: Al2O3, alumina, aluminium oxide, aluminum oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.48 g/cc0.126 lb/in³
Water Absorption 0.00 %0.00 %
Open Porosity 0.00 %0.00 %Gas tight. Test with helium mass spectrometer
Weibull Modulus 6.06.0
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 880880KHN5 microhardness, kg/mm²
Vickers Microhardness 985985HV5 microhardness, kg/mm²
Tensile Strength, Ultimate 124 MPa18000 psiACMA Test #4
Modulus of Elasticity 248 GPa36000 ksiultrasonic
Compressive Strength 1600 MPa232000 psiASTM C773-74
Poissons Ratio 0.200.20ASTM C623
Fracture Toughness 3.90 MPa-m½3.55 ksi-in½Kic (indentation)
Shear Modulus 103 GPa14900 ksiultrasonic
 
Thermal PropertiesMetricEnglishComments
CTE, linear  5.10 µm/m-°C
@Temperature 25.0 - 200 °C
2.83 µin/in-°F
@Temperature 77.0 - 392 °F
ASTM C32
 6.50 µm/m-°C
@Temperature 25.0 - 500 °C
3.61 µin/in-°F
@Temperature 77.0 - 932 °F
ASTM C32
 7.50 µm/m-°C
@Temperature 25.0 - 800 °C
4.17 µin/in-°F
@Temperature 77.0 - 1470 °F
ASTM C32
 8.00 µm/m-°C
@Temperature 25.0 - 1000 °C
4.44 µin/in-°F
@Temperature 77.0 - 1830 °F
ASTM C32
Thermal Conductivity 21.0 W/m-K146 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 87 %87 %
 
Descriptive Properties
ColorOff White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
Overview - Alumina, 98%, Al2O3
Aluminum, Al
Aluminum 1050-H14
Ferro Aluminum Oxide Grinding Media P70

CFC007 / 805

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.