MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Axiall Suprel® SVA 9412 Rigid PVC, Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Georgia Gulf Suprel® SVA 9412 injection molding alloy features excellent impact resistance, excellent processing characteristics and comprehensive UL listings. The UL listings of Suprel 9412 include elevated Relative Thermal Index ratings, weatherability listings per UL 746C and good flammability listings.

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D-792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inASTM D-955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 32.4 MPa4700 psiASTM D-638
Tensile Modulus 1.93 GPa280 ksiASTM D-638
Flexural Strength 50.3 MPa7300 psiASTM D-790
Flexural Modulus 1.72 GPa250 ksiASTM D-790
Izod Impact, Notched  1.60 J/cm
@Thickness 3.17 mm,
Temperature -40.0 °C
3.00 ft-lb/in
@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D-256
 8.01 J/cm
@Thickness 3.17 mm,
Temperature 22.8 °C
15.0 ft-lb/in
@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D-256
Gardner Impact 0.102 J
@Thickness 1.59 mm,
Temperature -40.0 °C
0.0750 ft-lb
@Thickness 0.0625 in,
Temperature -40.0 °F
per mil; ASTM D-4226
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °Funannealed; ASTM D-648
 81.00 °C177.8 °Fannealed; ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 66.00 °C150.8 °Funannealed; ASTM D-648
 80.0 °C176 °Fannealed; ASTM D-648
Vicat Softening Point 88.3 °C191 °Fannealed; ASTM D-1525A
UL RTI, Electrical 95.0 °C203 °FUL-746B
UL RTI, Mechanical with Impact 85.0 °C185 °FUL-746B
UL RTI, Mechanical without Impact 95.0 °C203 °FUL-746B
Flammability, UL94  V-0
@Thickness 2.54 mm
V-0
@Thickness 0.100 in
 5VA
@Thickness 2.00 mm
5VA
@Thickness 0.0787 in
 
Descriptive Properties
UL Weatherability Rating F(1)/F(2)UL-746C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fir, Subalpine
Axiall 1601 Clear 7002 Flexible PVC
Axiall 8150 Rigid PVC, Extrusion & Molding
Colorite Polymers 2019F Rigid PVC
Novatec Novablend® 4545 PVC

PGGUL483 / 41759

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.