MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow VORANOL™ VORACTIV™ 6340 Catalytically Active Polyether Polyol
Categories: Polymer; Thermoset

Material Notes: VORANOL™ VORACTIV™ 6340 polyether polyol is a catalytically active, high functionality capped polyol. Its high molecular weight, functionality, high primary hydroxyl content, and inherent catalytic activity make it well suited for high-resilience, flexible molded foams. These foams may be made utilizing TDI, TDI/MDI blends, or all-MDI isocyanate compositions.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/cc
Density 1.02 g/cc0.0368 lb/in³
Viscosity Measure 600 - 700 cSt
@Temperature 37.8 °C
600 - 700 cSt
@Temperature 100 °F
Maximum Moisture Content 0.0800.080
Vapor Pressure <= 0.000133 bar<= 0.100 torr
ASTM Color <= 75<= 75APHA
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity  1.84 J/g-°C
@Temperature 20.0 °C
0.440 BTU/lb-°F
@Temperature 68.0 °F
 2.00 J/g-°C
@Temperature 60.0 °C
0.478 BTU/lb-°F
@Temperature 140 °F
 2.09 J/g-°C
@Temperature 100 °C
0.500 BTU/lb-°F
@Temperature 212 °F
Thermal Conductivity 0.163 W/m-K1.13 BTU-in/hr-ft²-°F
 0.155 W/m-K
@Temperature 100 °C
1.07 BTU-in/hr-ft²-°F
@Temperature 212 °F
 0.159 W/m-K
@Temperature 50.0 °C
1.10 BTU-in/hr-ft²-°F
@Temperature 122 °F
Flash Point >= 204 °C>= 399 °FPMCC
 
Descriptive Properties
Hydroxyl Number mg KOH/g30 - 34

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow VORANOL™ CP 4711 Polyol
Dow VORANOL™ CP 1421 Polyol
Dow VORANOL™ CP 755 Polyol
Dow SPECFLEX™ NC 632 Polyol
Dow VORANOL™ CP 6001 Polyol

PDOW1483 / 30701

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.