MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

NuSil R-2930 Silicone, Thermally Conductive
Categories: Polymer; Thermoset; Silicone

Material Notes: General Purpose: Thermally Conductive

Cure System: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.55 g/cc1.55 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080
Tensile Strength at Break 1.72 MPa249 psi
Elongation at Break 20 %20 %
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 34.6 kV/mm880 kV/in
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.46 W/m-K10.1 BTU-in/hr-ft²-°FASTM E1530
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min
@Temperature 150 °C
0.500 hour
@Temperature 302 °F
Working Life 180 min180 min
 
Descriptive Properties
ColorWhite
Mix Ratio15:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUCON PX-9002 Thermally Conductive Thermoplastic
LG Chemical LUCON PL-9000 Thermally Conductive Thermoplastic
LG Chemical LUCON PX-9007 Thermally Conductive Thermoplastic
NuSil CV-2900 Silicone, Thermally Conductive
NuSil CV-2942 Silicone, Thermally Conductive

PNUSIL072 / 141796

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.