MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Manganese-Aluminum Bronze, UNS C95700, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, Permanent Mold, Plaster, and Sand.

Applications: Propellers, impellers, stator clamp segments, safety tools, welding rods, valves, pump castings.

Classified under: Aluminum bronzes

Data typical for sand-cast test bars. Alloy does not respond to heat treating

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.53 g/cc0.272 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 1801803000 kg
Hardness, Rockwell B 85 - 9085 - 90as cast or cast and annealed
Tensile Strength, Ultimate 620 MPa89900 psi
Tensile Strength, Yield 275 MPa39900 psi
Elongation at Break 20 %20 %in 50 mm
Reduction of Area 24 %24 %
Creep Strength  31.0 MPa
@Temperature 290 °C
4500 psi
@Temperature 554 °F
for 0.00001%/h
 66.0 MPa
@Temperature 205 °C
9570 psi
@Temperature 401 °F
for 0.00001%/h
 39.0 MPa
@Temperature 370 °C,
Time 3.60e+8 sec
5660 psi
@Temperature 698 °F,
Time 100000 hour
for 0.00001%/h
 232 MPa
@Temperature 260 °C,
Time 3.60e+8 sec
33600 psi
@Temperature 500 °F,
Time 100000 hour
for 0.00001%/h
 470 MPa
@Temperature 205 °C,
Time 3.60e+8 sec
68200 psi
@Temperature 401 °F,
Time 100000 hour
for 0.00001%/h
Modulus of Elasticity 125 GPa18100 ksi
Compressive Strength 1035 MPa150100 psias cast, at permanent set of 0.1%
Poissons Ratio 0.3260.326
Fatigue Strength 231 MPa
@# of Cycles 1.00e+8
33500 psi
@# of Cycles 1.00e+8
Reverse Bending
Machinability 50 %50 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 44.0 GPa6380 ksi
Izod Impact 27.0 J
@Temperature 20.0 °C
19.9 ft-lb
@Temperature 68.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000556 ohm-cm0.0000556 ohm-cm
Magnetic Permeability 1.031.03Demagnetized (annealed, fast cooled)
 2.2 - 152.2 - 15Magnetic condition (as-cast, slow cooled)
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.78 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.400 J/g-°C0.0956 BTU/lb-°F
Thermal Conductivity 12.1 W/m-K
@Temperature 20.0 °C
84.0 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 950 - 990 °C1740 - 1810 °F
Solidus 950 °C1740 °F
Liquidus 990 °C1810 °F
Shrinkage 1.6 %1.6 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 620 °C1150 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 7.0 - 8.5 %7.0 - 8.5 %
Copper, Cu 75 %75 %
Iron, Fe 2.0 - 4.0 %2.0 - 4.0 %
Lead, Pb <= 0.030 %<= 0.030 %
Manganese, Mn 11 - 14 %11 - 14 %
Nickel, Ni 1.5 - 3.0 %1.5 - 3.0 %
Other, total <= 0.50 %<= 0.50 %
Silicon, Si <= 0.10 %<= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alpha Nickel-Aluminum Bronze, UNS C95800, Copper Casting Alloy
Aluminum Bronze, UNS C95200, Copper Casting Alloy
Copper, UNS C62400 (Aluminum Bronze 11%)
High-Leaded Tin Bronze, UNS C93900, Copper Casting Alloy
Aluminum-Silicon Bronze, UNS C95600, Copper Casting Alloy

MC95700b1 / 11967

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.