MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Bynel® 40E529 Anhydride-Modified HDPE Adhesive Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Anhydride-Modified Polyethylene; High Density (HDPE)

Material Notes: Bynel® Series 4000 resins are anhydride-modified, high-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins.

Applications: Bynel® Series 4000 resins are excellent moisture barriers and have a good hydrocarbon resistance. This unique combination of properties makes them useful in a variety of coextrusion applications. HDPE/EVOH tubing and HDPE/polyamide bottles for agricultural chemicals are two examples. Bynel® Series 4000 resins adhere to a variety of materials. They are most often used in coextrusion with EVA, EVOH, polyamide, and PE. Bynel® 4003 is suitable for blown film with polyamide. Bynel® 4006 is appropriate for coextrusion blow molding with either polyamide or EVOH. Bynel® 40E529 can be used for extrusion coating onto paper or bonding to metal surfaces. It provides strong bonds to nylon and good bonds to EVOH in blown film, cast film, and pipe extrusion processes.

Physical properties of Bynel® Series 4000 resins are typical of high-density polyethylene resins with similar density and melt index values. The rheology characteristics of each grade are different, so one may be better suited than the others to a particular extrusion process.

Information provided by DuPont Packaging Polymers.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.935 g/cc0.0338 lb/in³ASTM D792
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Thermal PropertiesMetricEnglishComments
Melting Point 117 °C243 °FFreezing point via DSC/ASTM D3418
 135 °C275 °FMelting point via DSC/ASTM D3418
Vicat Softening Point 119 °C246 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 235 °C455 °FExtruder forward zone and adapter for film or coating with EVA or EVOH
Nozzle Temperature 235 °C455 °FDie

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Bynel® 4104 Anhydride-Modified LLDPE Adhesive Resin
Dow Bynel® 4105 Anhydride-Modified LLDPE Adhesive Resin
Dow Bynel® 39E660 Adhesive Resin
Dow Bynel® 30E671 Adhesive Resin
Dow Bynel® 30E670 Adhesive Resin

PDUPBS / 33573

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.