MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Guarniflon PTFE G455 Polytetrafluoroethylene 35% Carbographite
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Conductive Carbon Filled

Material Notes: PTFE G Special Compound with carbon..
Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high wear strength. Enhanced chemical resistance
Applications: Bearings for high speed and when fast dissipation of electric charges is needed. Elastic bands for unlubricated compressors. Valve seats.

Information provided by Guarniflon®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.90 - 2.00 g/cc0.0686 - 0.0723 lb/in³molded; ASTM D792
Deformation  4.0 - 6.0 %
@Pressure 13.7 MPa,
Time 86400 sec
4.0 - 6.0 %
@Pressure 1990 psi,
Time 24.0 hour
after 24hr relaxation; ASTM D621
 12 - 13.5 %
@Pressure 13.7 MPa,
Time 86400 sec
12 - 13.5 %
@Pressure 1990 psi,
Time 24.0 hour
ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 65 - 7065 - 70molded; ASTM D2240
Tensile Strength 8.00 - 13.0 MPa1160 - 1890 psimolded; ASTM D4745
Elongation at Break 40 - 70 %40 - 70 %molded; ASTM D4745
Compressive Yield Strength 12.0 - 13.5 MPa
@Strain 1 %
1740 - 1960 psi
@Strain 1 %
ASTM D695
Coefficient of Friction, Dynamic 0.120.12
K (wear) Factor 20.0 - 30.0 x 10-8 mm³/N-M9.93 - 14.9 x 10-10 in³-min/ft-lb-hrat PV 100; ASTM D3702
 
Thermal PropertiesMetricEnglishComments
CTE, linear 65.0 - 100 µm/m-°C36.1 - 55.6 µin/in-°FASTM D696
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -200 °C-328 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Omnia Plastica PTFE Polytetrafluoroethylene
Overview of materials for Polytetrafluoroethylene (PTFE), Carbon Fiber Filled
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled
Beijing Evergrow Resources PTFE, 20% Glass Fiber, 5% Graphite Filled
Overview of materials for Polyetheretherketone, PTFE Filled

PGUARN017 / 142750

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.