MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Sarlink® TPV 22035N Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 22035N is a highly engineered thermoplastic vulcanizate that can also be used as a compound matserbatch for use in demanding automotive and industrial applications. This product is a low hardness, low density grade with exceptional tensile strength, superior compression set, chemical resistance and high temperature performance. It can be easily processed by injection molding, blow molding or extrusion for various applications such as boots and bellows, seals, gaskets as well as other profiles and articles.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Processability; High Heat Resistance; High Tensile Strength; Low Compression Set; Low Density; Low Specific Gravity; Low Hardness

Uses: Automotive Applications; Constant Velocity Joint Boots; Gaskets; Industrial Applications; Profiles; Rubber Replacement; Seals

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 g/cc0.0333 lb/in³ISO 1183
Viscosity 300 cP
@Shear Rate 206 1/s,
Temperature 200 °C
300 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  39
@Time 5.00 sec
39
@Time 0.00139 hour
Extruded; ASTM D2240
 41
@Time 5.00 sec
41
@Time 0.00139 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 2.40 MPa348 psiFlow; ISO 37
 3.40 MPa493 psiAcross Flow; ISO 37
 3.33 MPa
@Treatment Temp. 150 °C,
Time 605000 sec
483 psi
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 3.60 MPa
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
523 psi
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain  1.00 MPa
@Strain 100 %
145 psi
@Strain 100 %
Across Flow; ISO 37
 2.10 MPa
@Strain 100 %
305 psi
@Strain 100 %
Flow; ISO 37
 1.03 MPa
@Strain 100 %,
Treatment Temp. 150 °C
149 psi
@Strain 100 %,
Treatment Temp. 302 °F
Across Flow, Change in Air at 168 hr; ISO 188
 1.05 MPa
@Strain 100 %,
Treatment Temp. 135 °C
152 psi
@Strain 100 %,
Treatment Temp. 275 °F
Across Flow, Change in Air at 1000 hr; ISO 188
Elongation at Break 160 %160 %Flow; ISO 37
 480 %480 %Across Flow; ISO 37
 557 %
@Treatment Temp. 150 °C,
Time 605000 sec
557 %
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 600 %
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
600 %
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
Tear Strength 11.0 kN/m63.0 pliMethod Ba, Angle (Unnicked), Across Flow; ISO 34-1
Compression Set  12 %
@Temperature 22.8 °C,
Time 79200 sec
12 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 21 %
@Temperature 70.0 °C,
Time 79200 sec
21 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 37 %
@Temperature 125 °C,
Time 252000 sec
37 %
@Temperature 257 °F,
Time 70.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Processing Temperature 182 - 221 °C360 - 430 °FInjection, Melt
Rear Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Middle Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Front Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Nozzle Temperature 188 - 221 °C370 - 430 °FInjection
Zone 1 182 - 204 °C360 - 400 °FExtrusion
Zone 2 182 - 204 °C360 - 400 °FExtrusion
Zone 3 188 - 210 °C370 - 410 °FExtrusion
Zone 4 188 - 210 °C370 - 410 °FExtrusion
Die Temperature 193 - 216 °C380 - 420 °FExtrusion
Melt Temperature 193 - 216 °C380 - 420 °F
Mold Temperature 10.0 - 65.6 °C50.0 - 150 °FInjection
Drying Temperature 82.2 °C180 °F
Dry Time 3.00 hour3.00 hour
Back Pressure 0.0689 - 1.03 MPa10.0 - 150 psiInjection
Screw Speed 100 - 200 rpm100 - 200 rpmInjection
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alliance Polymers Viprene™ G45A-32U-BLK Thermoplastic Vulcanizate Elastomer
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer
Barlog Plastics KEBAFLEX E 50.1 TPE-V, Shore A50
Teknor Apex Sarlink® TPV 3470N Thermoplastic Vulcanizate

PTEKNQ1181 / 237672

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.