MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® 914 175°C Curing Epoxy Matrix
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: HexPly® 914 is a highly successful modified epoxy matrix which is used extensively in high temperature resistant primary aircraft structures. The controlled melt viscosity and excellent matrix rheology of 914 permits a wide range of processing conditions for high quality components.

Features: High melt viscosity giving easy processing characteristics, Tolerant to a wide variation of processing conditions, Latitude for low to high pressure laminating or moulding processes, Medium tack level giving excellent drape characteristics, Good shelf life

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³Cured
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 47.7 MPa6920 psiISO R527 type 1
Elongation at Yield 1.5 %1.5 %ISO R527 type 1
Tensile Modulus 3.90 GPa566 ksiISO R527 type 1
Compressive Yield Strength 180 MPa26100 psiISO 604
Poissons Ratio 0.410.41ISO R527 type 1
Fracture Toughness 0.700 MPa-m½0.637 ksi-in½
Shear Modulus 1.40 GPa203 ksiISO R527 type 1
Toughness 103 J76.0 ft-lbPer square meter
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 190 °C374 °FDMTA
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature -18.0 °C
12.0 Month
@Temperature -0.400 °F
 
Descriptive Properties
Tack Life (days)60

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® 8552 Epoxy Matrix
Hexcel® HexPly® 1454 125°C Curing Epoxy Matrix
Hexcel® HexPly® 171/174/176 120°C Curing Epoxy Matrix
Hexcel® HexPly® 6376 175°C Curing Epoxy Matrix
Hexcel® HexPly® 913 125°C Curing Epoxy Matrix

PHEXC059 / 98529

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.