MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese AT 195 Low Density Polyethylene (LDPE)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: AT 195 resin is suitable for use in hot melt adhesive and coating applications. It complies with Code of Federal Regulation 21 CFR Section 177.1520 subject to extraction limitations for specific end use applications. Additives:

Applications: Adhesives & Sealants

Information provided by Celanese Corporation.

Key Words: hot melt coating and adhesive applications
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ASTM D1505; ASTM D1928 Proc C Mod
Melt Flow 2300 g/10 min
@Load 0.325 kg,
Temperature 125 °C
2300 g/10 min
@Load 0.716 lb,
Temperature 257 °F
Modified; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9393ASTM D2240
Hardness, Shore D 4242ASTM D2240
Tensile Strength at Break 5.60 MPa812 psiType IV (50 mm/min); ASTM D638
Elongation at Break 65 %65 %Type IV (50 mm/min); ASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 95.0 °C203 °FDSC; ASTM D3417
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Molded
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
Celanese AT 253 Low Density Polyethylene (LDPE)
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade
Overview of materials for Medium Density Polyethylene (MDPE), Molded

PATEVB21 / 25977

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.