MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem IF33 LLDPE Injection Molding Polyethylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Extrusion Grade; LLDPE/Octene, Extruded; LLDPE/Hexene, Molded

Material Notes: IF33 is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high fluidity, good flexibility, and low warpage. It contains antioxidant additives. This resin has been specifically developed for injection molding lid seals and lids for food containers, housewares, containers, and general purpose. IF33 has been developed to be used in the injection molding process under conditions comparable to linear low-density polyethylene. Recommended temperature profile: 150 to 210ºC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.931 g/cc0.0336 lb/in³ASTM-D729
ESCR 10% Igepal® <= 1.0 hour
@Thickness 2.00 mm,
Temperature 50.0 °C
<= 1.0 hour
@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Melt Flow 48 g/10 min
@Load 2.16 kg,
Temperature 190 °C
48 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5151ASTM-D2240
Tensile Strength at Break 9.00 MPa1310 psiASTM-D638
Tensile Strength, Yield 15.0 MPa2180 psiASTM-D638
Elongation at Break 100 %100 %ASTM-D638
Elongation at Yield 14 %14 %ASTM-D638
Modulus of Rigidity 0.490 GPa71.1 ksiASTM-D747
Flexural Modulus, 1% Secant 543 MPa78800 psiASTM-D790
Izod Impact, Notched 0.900 J/cm1.69 ft-lb/inASTM-D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 46.0 °C115 °FASTM-D648
Vicat Softening Point 97.0 °C
@Load 1.02 kg
207 °F
@Load 2.25 lb
ASTM-D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DNDA-9810 NT 7 Linear Low Density Polyethylene Resin
Dow DOWLEX™ 2505 Linear Low Density Polyethylene, Narrow MW Distribution
Braskem RP 347 Injection Molding Polypropylene
Braskem H 502 HC Injection Molding Polypropylene
Braskem CP 401 HC Injection Molding Polypropylene

PBRAS909 / 106755

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.