MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Goodfellow Carbon-Carbon Composite
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite

Material Notes: Carbon Fiber - Carbon Matrix

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 - 1.80 g/cc0.0470 - 0.0650 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break <= 10.0 MPa<= 1450 psiTransverse
 40.0 - 70.0 MPa5800 - 10200 psiLongitudinal
Tensile Modulus 20.0 - 30.0 GPa2900 - 4350 ksiParallel to Plane
Flexural Strength 80.0 - 200 MPa11600 - 29000 psiParallel to Plane
Flexural Modulus 10.0 - 20.0 GPa1450 - 2900 ksiParallel to Plane
Compressive Strength 60.0 - 150 MPa8700 - 21800 psiPerpendicular to Plane
 120 - 200 MPa17400 - 29000 psiParallel to Plane
Shear Strength 20.0 - 30.0 MPa2900 - 4350 psiin Plane
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00300 ohm-cm0.00300 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 1.50 µm/m-°C
@Temperature 20.0 - 1000 °C
0.833 µin/in-°F
@Temperature 68.0 - 1830 °F
CTE, linear, Transverse to Flow  6.00 µm/m-°C
@Temperature 20.0 - 1000 °C
3.33 µin/in-°F
@Temperature 68.0 - 1830 °F
 6.00 µm/m-°C
@Temperature 20.0 - 1000 °C
3.33 µin/in-°F
@Temperature 68.0 - 1830 °F
Thermal Conductivity 50.0 - 100 W/m-K347 - 694 BTU-in/hr-ft²-°FPerpendicular to Plane
 250 - 300 W/m-K1740 - 2080 BTU-in/hr-ft²-°FParallel to Plane

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carlisle 201HD Carbon-Carbon Composite
Carlisle 201HL Carbon-Carbon Composite
Carlisle 201LD Carbon-Carbon Composite
Carlisle 201LL Carbon-Carbon Composite
Solvay Thornel® T-300 1K Carbon Fiber, Polyacrylonitrile (PAN) Precursor

PGOODF116 / 42271

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.