MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Elastollan® C-64D Polyester Type Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Recommended for injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fuel and solvent resistance. These products can be injection and blow molded and extruded.

As with all TPU products this grade must be dried prior to processing.

Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.

Key Words: TPU Rubbers
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6464ASTM D2240
Tensile Strength, Ultimate 40.0 MPa5800 psiASTM D412
Tensile Stress at Strain  26.0 MPa
@Strain 100 %
3770 psi
@Strain 100 %
ASTM D-412
 38.0 MPa
@Strain 300 %
5510 psi
@Strain 300 %
ASTM D-412
Elongation at Break 430 %430 %ASTM D412
Modulus of Elasticity 0.400 GPa58.0 ksi
Shear Modulus 0.250 GPa36.3 ksi
Tear Strength 220 kN/m1260 pliASTM D624
Taber Abrasion, mg/1000 Cycles 5050H-18 wheel; ASTM D-1044.
Tensile Set 100 %100 %at break; ASTM D-412
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmDIN 53482/VDE 0303
Surface Resistance >= 1.00e+12 ohm>= 1.00e+12 ohmDIN 53482/VDE 0303
Dielectric Constant  4.1
@Frequency 1e+6 Hz
4.1
@Frequency 1e+6 Hz
DIN 53483/VDE 0303
 4.8
@Frequency 1000 Hz
4.8
@Frequency 1000 Hz
DIN 53483/VDE 0303
 5.1
@Frequency 50 Hz
5.1
@Frequency 50 Hz
DIN 53483/VDE 0303
Dielectric Strength >= 49.0 kV/mm>= 1240 kV/inDIN 53481/VDE 0303
Dissipation Factor  0.031
@Frequency 1000 Hz
0.031
@Frequency 1000 Hz
 0.034
@Frequency 50 Hz
0.034
@Frequency 50 Hz
 0.045
@Frequency 1e+6 Hz
0.045
@Frequency 1e+6 Hz
Comparative Tracking Index >= 600 V>= 600 VDIN/IRC 112
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 165 °C329 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Elastollan® C-85A Polyester Type Polyurethane Elastomer
BASF Elastollan® 1195A Polyether Type Polyurethane Elastomer
BASF Elastollan® 1185A Polyether Type Polyurethane Elastomer
BASF Elastollan® C-95A Polyester Type Polyurethane Elastomer
BASF Elastollan® S60D Polyester Type Polyurethane Elastomer

PSF971 / 67187

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.