MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mytex Polymers AS319LW-01US Thermoplastic Polyolefin, 19% Talc Filled
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polyolefin

Material Notes: AS319LW-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural, generic black or pre-colored for partial paint applications.
Key Applications: Exterior Parts-Bumper Fascia, Cladding
OEM Approvals: Chrysler MS-DC 256 Type C, CPN 3059 (MIC), CPN 4538 (Paint) CP 112

Information provided by Mytex Polymers

Key Words: TPO
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ISO 1183 A
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/in48 hours after molding; ISO 294-3/4
 0.0060 - 0.0080 cm/cm
@Time 3600 sec
0.0060 - 0.0080 in/in
@Time 1.00 hour
48 hours after molding; ISO 294-3/4
 0.0070 - 0.0090 cm/cm
@Time 3600 sec
0.0070 - 0.0090 in/in
@Time 1.00 hour
48 hours after molding; ISO 294-3/4
Melt Flow 24 g/10 min
@Load 2.16 kg,
Temperature 230 °C
24 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133 B
Ash 19 %
@Temperature 600 °C
19 %
@Temperature 1110 °F
ISO 3451/1A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 17.0 MPa2470 psiISO 527-1/1A/50
Flexural Modulus 1.70 GPa247 ksiChord, 2mm/min; ISO 178
Izod Impact, Notched (ISO) 46.0 kJ/m²
@Temperature 23.0 °C
21.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1eA
Dart Drop, Total Energy 16.0 J
@Temperature 23.0 °C
11.8 ft-lb
@Temperature 73.4 °F
Multiaxial Impact Strength, Max Load, 2.2 m/s; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C216 °FMethod A, flatwise, unannealed; ISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °FMethod A, flatwise, unannealed; ISO 75-1/2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mytex Polymers AS319L-01US Thermoplastic Polyolefin, 19% Talc Filled
ExxonMobil PP8114E1 Impact Copolymer
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade
A. Schulman TPP20AF01HB 20% Talc-Filled Homopolymer Polypropylene
Cotronics Duralco™ 4538N Super Flexible Epoxy, Room Temperature Cure

PMYTEX033 / 104601

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.