MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celanex® 3300-2LM PBT, Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified

Material Notes: Celanex 3300-2LM is a 30% glass-filled PBT that is enhanced for improved laser marking graphics. It contains an internal lubricant for enhanced mold release. It is a lasermarkable grade available in a black color to mark white, The grade is specially formulated to yield crisp marks when subjected to a Nd:YAG laser or equivalent operated at 1064nm or 532nm. Lasers operating in the UV region (355nm) may yield different results

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.53 g/cc0.0553 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9090ISO 2039-2
Tensile Strength at Break 130 MPa18900 psi5mm/min; ISO 527-2/1A
 134 MPa19500 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Flexural Strength 193 MPa28000 psiASTM D790
 210 MPa30500 psiISO 178
Flexural Modulus 9.70 GPa1410 ksiISO 178
Izod Impact, Notched 0.908 J/cm1.70 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 7.50 kJ/m²3.57 ft-lb/in²ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 228 °C442 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 206 °C403 °FASTM D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 65.0 - 93.0 °C149 - 199 °Fcavity
 250 - 260 °C482 - 500 °Fhot runner
Feed Temperature 230 - 240 °C446 - 464 °F
Zone 1 230 - 240 °C446 - 464 °F
Zone 2 235 - 250 °C455 - 482 °F
Zone 3 235 - 250 °C455 - 482 °F
Zone 4 240 - 260 °C464 - 500 °F
Die Temperature 250 - 260 °C482 - 500 °F
Melt Temperature 235 - 260 °C455 - 500 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Novaduran® 5010GN6-30M8X Polybutylene Terephthalate
Mitsubishi Novaduran® 5010GN6-30T Polybutylene Terephthalate
Celanese Celanex® 3300-2FC PBT, 30% Glass Reinforced
Celanese Celanex® 3300 PBT, 30% Glass Reinforced
Celanese Celanex® 3300-2 PBT, 30% Glass Reinforced

PHCQ049 / 178504

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.