MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostacom G3 U01 L Polypropylene, Glass/Mineral Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: Hostacom G3 U01 L is a glass fiber reinforced PP homopolymer with medium melt flow rate. Product is UL certified in all color.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 1183-1A
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 230 °C
15 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 95.0 MPa13800 psiISO 527-1,-2
Elongation at Yield 3.0 %3.0 %ISO 527-1,-2
Tensile Modulus 6.80 GPa986 ksiISO 527-1,-2
Flexural Modulus 5.60 GPa812 ksiTech.A; ISO 178/A1
Charpy Impact Unnotched 4.00 J/cm²19.0 ft-lb/in²ISO 179-1/1eU
Charpy Impact, Notched 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 155 °C311 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 145 °C293 °FISO 75-1,-2
Vicat Softening Point 135 °C275 °FB50N; ISO 306
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostacom G3 U01 102297 Polypropylene with 30% Glass Fiber Filler
LyondellBasell Hostacom G3 N01 L Polypropylene with 30% Glass Fiber Filler
Avient Maxxam™ FR 8000 Polypropylene with 30% Glass Fiber
LyondellBasell Hostacom G3 N01 102297 Polypropylene with 30% Glass Fiber Filler
LyondellBasell Hostacom 5115 2003 (SC BLACK) Polypropylene with 30% Glass Fiber Filler

PEQT7947 / 219584

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.