MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow DOWLEX™ 3010 Linear Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: DOWLEX® 3010 Polyethylene resin is a polyethylene polymer designed to offer high performance properties such as excellent environmental stress crack resistance, tear strength, abrasion resistance, and strong heat seals in thin extrusion coatings. It has good processability over a wide range of molding conditions. This material complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.2 for food contact applications and with regulation 177.1390 c (1) (I) (a) for high temperature laminates. The regulations should be consulted for complete details.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 g/cc0.0333 lb/in³
Melt Flow 5.5 g/10 min
@Load 2.16 kg
5.5 g/10 min
@Load 4.76 lb
Melt flow ratio I10/I2 is 7.5.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 14.5 MPa2100 psi
Tensile Strength, Yield 12.4 MPa1800 psi
Elongation at Break 720 %720 %
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DOWLEX™ IP-2580 Linear Low Density Polyethylene
Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade
Dow DOWLEX™ 2045.11 Linear Low Density Polyethylene, Heavy Duty Film Grade
Dow DOWLEX™ 2517 Linear Low Density Polyethylene, Narrow MW Distribution
Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade

PDW456 / 34525

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.