MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bales Mold Service Nibore® Electroless Nickel - Boron Nitride Mold Coating
Categories: Metal; Nonferrous Metal; Nickel Alloy; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Nibore® is an electroless nickel phosphorus coating that incorporates boron nitride particles in a co-deposited nickel matrix. This unique process is formulated to produce a uniformly dispersed boron nitride deposit. Nibore™ boasts a 54 RC hardness, which can be increased to 67 RC after heat treating. The additional hardness adds to the unique capabilities of this engineered coating treatment. The extremely low coefficient of friction has proven valuable in high wear applications where galling and release are an issue. With a working temperature of 1250°F, this deposit will perform in the most extreme applications.

Information provided by Bales Mold Service.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.10 g/cc0.293 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 5454As Plated
 6767After Heat Treatment at 550°F
Coefficient of Friction <= 0.05<= 0.05
 
Thermal PropertiesMetricEnglishComments
Melting Point 899 °C1650 °F
Maximum Service Temperature, Air 677 °C1250 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 85.0 °C185 °FApplied Temperature
 
Descriptive Properties
Phosphorus Content4-6 wt.%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allvac® Nickelvac® N-90 Nickel Superalloy, Heat Treatment: 1066°C (1950°F) + Age
California Fine Wire Stablohm 710 Nickel Chromium Resistance Wire
Overview of materials for Aluminum Alloy
3M Techical Ceramics EKagrip® 10 Friction-enhancing electroless nickel diamond coating
Kennametal Stellite Nucalloy® 41 Nickel-Chromium-Boron Alloy

NBAL6 / 15085

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.