MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco AREMCOLOX™ 502-1900-YTZP Dense Yttria Stabilized Zirconium Oxide
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: This grade offers the highest flexural strength of all the zirconia materials. The fine grain size lends itself to be used in cutting tools where a very sharp edge can be achieved and maintained due to its high wear resistance. Also provides excellent mechanical strength, corrosion and thermal shock resistance, impact toughness, and very low thermal conductivity. Used for structural components, wear parts, fiber optic ferrules and sleeves, oxygen sensors, solid oxide fuel cells.

Key Words: YSZ, ZrO2
Vendors: Aremco offers a range of adhesives formulated using a broad range of ceramics fillers and inorganic binders, and are ideal for bonding, potting and sealing ceramics, composites, graphite, refractory metals, quartz, and semiconductors. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 6.02 g/cc6.02 g/cc
Water Absorption 0.00 %0.00 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 808045N
Flexural Strength 951 MPa138000 psi
Compressive Strength 2480 MPa360000 psi
Fracture Toughness 10.0 MPa-m½9.10 ksi-in½
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cm
Dielectric Constant 30
@Frequency 1e+6 Hz
30
@Frequency 1e+6 Hz
Dielectric Strength 9.45 kV/mm240 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.84 µm/m-°C3.80 µin/in-°F
Thermal Conductivity 2.20 W/m-K15.3 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 499 °C930 °F
 
Descriptive Properties
ColorIvory
Gas permeabilityGas Tight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 7039-T64
Anderman Ceramics EM80P Corundum
MarkeTech Repton 868 Zirconia + 8 mol% Yttria (YSZ)
Anderman Ceramics EZY 94 Zirconia, 94%, Yttria-Stabilized
MarkeTech Ceraflex 3Y Thin Zirconia Ceramic, Yttria Stabilized

CAREM10h / 161697

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.