MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Betamate™ XW 1185 Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: BETAMATE™ XW 1185 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel and aluminum, is resistant to degradation and to substrate corrosion on environmental aging. The product is compatible with electro-coat paint process.

This former Dow product line is now a DuPont product line. Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ISO 1183
Solids Content >= 99 %>= 99 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 0.740 GPa107 ksiISO 527-1/-2
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month
@Temperature <=30.0 °C
3.00 Month
@Temperature <=86.0 °F
 
Descriptive Properties
BasisEpoxy resin
ColorGreen
CompatibilityMetals
Extrusion Viscosity6025°C, Ford nozzle d=3 mm / 3 bar
PolymerAdhesive

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow BETAMATE™ 1045 Epoxy
DuPont Mobility and Materials Betamate™ 1496V Epoxy Adhesive, Body Shop Grade
DuPont Mobility and Materials Betamate™ 5103-2 Epoxy Adhesive, Body Shop Grade
Dow BETAMATE™ 7000/7050 L Epoxy
DuPont BETAMATE™ 73345G Epoxy

PDTF9110 / 30219

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.