MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Momentive Performance Materials AC6043 Titanium Diboride/Boron Nitride Composite  (discontinued **)
Categories: Ceramic; Boride; Ceramic Matrix Composite; Nitride

Material Notes: TiB2/BN. Density is 83-92% of theoretical. Sonic Modular1 is 4 to 17 x 10^6 psi.

Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics, including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mullite and Titanium Diboride. This results in composites which are machinable, thermal shock resistant and chemically compatible in a wide range of environments. In combination with Titanium Diboride, for example, BN can be used as a heating source for the aluminum metallization of films and papers.

BN composites are also used:

Break-rings in the horizontal continuous castings of steel, and nozzles in rapid solidification processes

High temperature refractory shapes

Glass forming tools and refractories

Molds, dies and refractories for metalforming

Furnace vents, stacks and fixtures.

Information provided by Momentive Performance Materials, formerly GE Advanced Ceramics.

Key Words: BN, TiB2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 117 MPa17000 psi
 16.5 MPa
@Temperature 1500 °C
2390 psi
@Temperature 2730 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.00 - 6.00 µm/m-°C
@Temperature 20.0 °C
2.22 - 3.33 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 26.0 W/m-K180 BTU-in/hr-ft²-°F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ceradyne Ceralloy® 546-4E Boron Carbide
ExxonMobil Exxsol™ D30 Dearomatized Fluid
Momentive Performance Materials HCT-S Titanium Diboride (TiB2) Powder
H.C. Starck Grade HP Boron Carbide, B4C
Silicon Carbide, Reaction-Bonded, SiSiC

CADV48 / 432

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.