MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lehvoss LUVOCOM® 65-7311 PP-copolymer with carbon fiber
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Carbon Fiber Filled

Material Notes: Properties/attributes include: Strong, stiff parts. Electrically conductive, suitable for continuous discharging of statically-generated electricity. Low warpage.

Office communication.

Processing: During processing, the moisture content should not exceed 0.2%. Moisture may lead to smearing and in extreme cases to foaming. Usually the material can be processed over a broad temperature range and can thus be adapted to a wide variety of processing conditions. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccISO 1183
Moisture Absorption <= 0.300 %
@Temperature 23.0 °C,
Time 86400 sec
<= 0.300 %
@Temperature 73.4 °F,
Time 24.0 hour
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm0.0020 - 0.0060 in/inDIN 16901
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 54.0 MPa7830 psiISO 527-2
Elongation at Break 1.2 %1.2 %ISO 527-2
Modulus of Elasticity 7.00 GPa1020 ksiISO 527-2
Flexural Strength 78.0 MPa11300 psiISO 178
Flexural Modulus 6.00 GPa870 ksiISO 178
Flexural Strain at Break 1.5 %1.5 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched 3.50 J/cm²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eU
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 10.0 - 1.00e+7 ohm-cm10.0 - 1.00e+7 ohm-cmIEC 60167
Surface Resistance <= 1.00e+7 ohm<= 1.00e+7 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °FContinuous; UL 746B
 130 °C266 °FShort Term
Vicat Softening Point 80.0 °C176 °FVST A; DIN ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 220 - 250 °C428 - 482 °F
Zone 1 220 - 250 °C428 - 482 °F
Zone 2 220 - 250 °C428 - 482 °F
Zone 3 230 - 260 °C446 - 500 °F
Melt Temperature 230 - 260 °C446 - 500 °F
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature 70.0 - 95.0 °C
@Time 7200 - 14400 sec
158 - 203 °F
@Time 2.00 - 4.00 hour
Dehumidifying dryer
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI Latene® AG7H K/30 PP Homopolymer, 30% Carbon Fiber Reinforced, Heat Stabilized
MTI ThermoStran® PP-30C Long Carbon Fiber Compound
Overview of materials for Polypropylene, Carbon Fiber Filled
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced
RTP Company RTP 181 Polypropylene (PP); Carbon Fiber

PLUU8922 / 193881

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.