MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis Europrene® N 3345 Acrylonitrile-Butadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Europrene® N 3345 is a cold polymerized acrylonitrile-butadiene copolymer. A non staining antioxidant is added during the production process.

Key Features: Europrene® N 3345 is characterized by good processability, good mineral oil resistance and medium flexibility at low temperature. The vulcanization can be performed by sulphur based systems or by peroxides. The low temperature properties can be further improved by adding polar plasticizers as synthetic esters of adipic, sebacic or phthalic acids. To improve heat, light and ozone resistance, suitable protective agents as amine or phenolic antioxidants have to be added to the compounding process.

Main Applications: Wide range of oil resistant technical articles: seals, industrial shoes soles, seals, technical goods, etc.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Key Words: NBR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.70 %<= 0.70 %ASTM D5668
Mooney Viscosity 45
@Temperature 100 °C
45
@Temperature 212 °F
ASTM D1646
Ash <= 0.50 %<= 0.50 %ASTM D5667
 
Descriptive Properties
Acrylonitrile Content33% wtASTM D3533
Organic Acid< 0.5% wtASTM D5774
Soap< 0.6% wt

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Versalis Europrene® N 3345 GRN Acrylonitrile-Butadiene Rubber
Metflex M108 NBR 50; Acrylonitrile butadiene rubber with low-medium CAN content
Nitriflex NitriClean 3355 NBR - Nitrile Rubber
Versalis Europrene® N 3380 Acrylonitrile-Butadiene Rubber

PENG260 / 124654

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.