MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Visico™/Ambicat™ LE4421/LE4472 Ambient Curing, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Visico™ LE4421 / Ambicat™ LE4472 is a silane crosslinkable black compound designed for covering/insulation of overhead cables. The base material Visico™ LE4421 in combination with the catalyst masterbatch Ambicat™ LE4472 will accelerate the moisture-induced crosslinking reaction. The system is highly active and crosslinks quickly at ambient conditions, in sauna or in hot water. When properly mixed, addition of 7 parts of Ambicat™ LE4472 to 93 parts of Visico™ LE4421 , insulation with excellent thermo-oxidative stability, also in contact with copper as will as aluminum, is achieved. The final product will contain nominal 2,5% of fine size carbon black ensuring excellent weatherability. Applications: Covering/insulation of overhead cables. Additives: Visico™ LE4421 / Ambicat™ LE4472 contains antioxidant, metal deactivator and a drying agent. Visico™ LE4421 contains a permanent scorch retardant additive, ensuring safe processing and enabling the use of highly active crosslinking catalyst. Specifications: Visico™ LE4421 / Ambicat™ LE4472 in combination meets these applicable requirements when processed using sound extrusion and testing procedure: ANSI/ICEA S-70-547; ASTM D 1248 Type II, Class C, Category 4; HD 603 S1; HD 626 S1 (TIX-2, TIX-4, TIX-6, TIX-9); IEC 60502-1; NEMA WC 70; and NEMA WC 71.

Information provided by Borealis AG

Key Words: XLPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.933 g/cc0.0337 lb/in³ISO 1183/ISO 1872-2
ESCR 10% Igepal® >= 96 hour
@Temperature 50.0 °C
>= 96 hour
@Temperature 122 °F
F20; IEC 60811-4-1/B
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 52521s; ISO 868
Tensile Strength at Break <= 11.25 MPa<= 1632 psiafter aging (240h, 135°C); IEC 60811-1-2
 >= 15.0 MPa>= 2180 psi250mm/min; ISO 527
Elongation at Break >= 300 %>= 300 %250mm/min; ISO 527
Tensile Set 0.00 %
@Temperature 200 °C
0.00 %
@Temperature 392 °F
Permanent Deformation at 0.2 MPa after 60% elongation under load; IEC 60811-2-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+6 ohm-cm>= 1.00e+6 ohm-cmIEC 60093
Dielectric Constant 2.5
@Frequency 50000 Hz
2.5
@Frequency 50000 Hz
IEC 60250
Dielectric Strength >= 20.0 kV/mm>= 508 kV/inIEC 60243
Dissipation Factor 0.00060
@Frequency 50000 Hz
0.00060
@Frequency 50000 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -76.0 °C<= -105 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Zone 1 150 °C302 °F
Zone 2 170 °C338 °F
Zone 3 170 °C338 °F
Zone 4 170 °C338 °F
Die Temperature 170 °C338 °F
Shelf Life 15.0 Month15.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis LE4201R Polyethylene Insulation Compound, Crosslinkable
Borealis Borlink™ LS4201R Polyethylene Insulation Compound, Crosslinkable
Borealis Visico™/Ambicat™ LE4423/LE4472 Black, Fast Curing, Silane Crosslinkable LDPE Compound for Weather Resistant Covering/Insulation of Overhead Cables
Avient Syncure™ System S112NA Polyethylene, Crosslinked (XLPE)
Borealis Borlink™ LE4244R Polyethylene Insulation Compound, Crosslinkable

PBOREA600 / 108859

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.