MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company EMI 331 E FR Polycarbonate (PC) 10% Glass Fiber - Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Stainless Steel Fiber

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/ccASTM D 792
Additive Loading 10 %10 %Primary Additive
Linear Mold Shrinkage 0.0030 cm/cm
@Thickness 3.20 mm
0.0030 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 89.6 MPa13000 psiASTM D 638
Elongation at Break 3.0 %3.0 %ASTM D 638
Tensile Modulus 5.17 GPa750 ksiASTM D 638
Flexural Strength 145 MPa21000 psiASTM D 790
Flexural Modulus 4.96 GPa720 ksiASTM D 790
Izod Impact, Notched 0.801 J/cm
@Thickness 3.20 mm
1.50 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 5.34 J/cm
@Thickness 3.20 mm
10.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 10 ohm-cm<= 10 ohm-cmASTM D 257
Surface Resistance <= 1000 ohm<= 1000 ohmESD STM11.11
Surface Resistivity per Square <= 10000 ohm<= 10000 ohmASTM D 257; ESD STM11.11
Static Decay <= 2.0 sec<= 2.0 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
Shielding Effectiveness  42 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
42 dB
@Thickness 0.0787 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 43 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
43 dB
@Thickness 0.0787 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 44 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
44 dB
@Thickness 0.0787 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 46 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
46 dB
@Thickness 0.0787 in,
Frequency 1e+9 Hz
ASTM D 4935
 49 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
49 dB
@Thickness 0.0787 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 52 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
52 dB
@Thickness 0.0787 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 52 dB
@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
52 dB
@Thickness 0.118 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 53 dB
@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
53 dB
@Thickness 0.118 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 56 dB
@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
56 dB
@Thickness 0.118 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 60 dB
@Thickness 3.00 mm,
Frequency 1e+9 Hz
60 dB
@Thickness 0.118 in,
Frequency 1e+9 Hz
ASTM D 4935
 61 dB
@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
61 dB
@Thickness 0.118 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 61 dB
@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
61 dB
@Thickness 0.118 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 277 - 304 °C530 - 580 °F
Mold Temperature 71.1 - 121 °C160 - 250 °F
Drying Temperature 121 °C
@Time 14400 sec
250 °F
@Time 4.00 hour
Moisture Content 0.020 %0.020 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eurotec® Tecotek® PC43 GR10 BK002 PC, 10% glass fiber reinforced, black
Eurotec® Tecotek® PC40 GR10 NL PC, 10% glass fiber reinforced, natural
Cheng Yu Plastic ML3410 PC, 10% Glass Fiber
LG Chemical LUPOY SR-3108F High Flow Modified PC, 10% Mineral Fillers, High Reflectivity, Flame Retardant
Lavergne VYTEEN PCGF10BK PC 10% Glass Reinforced

PQZVA2889 / 120440

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.