MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Johnson Matthey HC Platinum w/ 5% Cobalt Jewelry Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Platinum Alloy

Material Notes: Fluid for hard castings. Cobalt has been used to create casting alloys at various levels of fineness. Cobalt suppresses oxygen level in the melt, improves fluidity and castability and gives a good final hardness without reducing the melting range significantly.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 20.8 g/cc0.751 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 135135Annealed
Elongation at Break 20 %20 %Annealed
 
Thermal PropertiesMetricEnglishComments
Melting Point 1750 - 1765 °C3180 - 3209 °F
Solidus 1750 °C3180 °F
Liquidus 1765 °C3209 °F
 
Component Elements PropertiesMetricEnglishComments
Cobalt, Co 5.0 %5.0 %
Platinum, Pt 95 %95 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Johnson Matthey GW Platinum w/ 5% Copper Jewelry Alloy
Johnson Matthey SW 950 Platinum w/ 5% Iridium Jewelry Alloy
CMW® ELKONIUM 32 platinum based alloy
CMW® ELKONIUM 306 platinum based alloy
CMW® ELKONIUM 305 platinum based alloy

NJMMJ63 / 97755

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.