MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Pulpsil® 355 Silicone Antifoam Compound
Categories: Fluid

Material Notes: Product description: A 100% active concentrated antifoam compound based on proprietary polysiloxane and silica technology. PULPSIL® 355 is an excellent formulation base for pulp and paper silicone emulsion defoamers. PULPSIL® 355 exhibits superior knockdown and holdout than most conventional silicone / silica defoamers. The antifoam agents active in PULPSIL® 355 are also matched with new organo-modified silicone glycol surfactants to provide improved drainage in most washing systems.

Application: PULPSIL® 355 is applicable in all types of pulping operations, but is particularly effective for kraft processes. Application is typically to the initial 2 to 3 stages of washing, with feed points to the stock inlet or dilution of the first stage, with smaller secondary applications to the subsequent stages. Feed rate generally ranges from 0.25 to 2.0 lb/ton of pulp. Actual product addition amounts and locations will depend on the needs of the individual processes.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
pH 7.07.0
Viscosity 1000 - 3500 cP1000 - 3500 cP
 
Descriptive Properties
Appearanceopaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Silfoam® SC 385 Silicone Antifoam Compound
Wacker Silfoam® SC 1132 Silicone Antifoam Compound
Dow 2210 ANTIFOAM
Dow Y-30 ANTIFOAM EMULSION
Quaker Quintolubric® 702-46 RD Water Glycol Hydraulic Fluid

PWACK9405 / 204934

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.