MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röhm Plexiglas® zk5HF Molding Compound
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes: PLEXIGLAS® Resist zk5HF is an amorphous, impact-modified thermoplastic molding compound (PMMA-I). Typical properties of impact-modified PLEXIGLAS® molding compounds are:
  • high weather resistance
  • excellent transmission and clarity
  • brilliant appearance
  • the pleasant feel and sound of the moldings
PLEXIGLAS® Resist zk5HF is characterized by the following special properties:
  • high break resistance and impact strength
  • improved resistance to stress cracking
  • excellent flow.
Application: Used for injection molding as well as for extruding sheets and profiles.

The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.50 %0.50 %23°C, 50%; ISO 62
Water Absorption at Saturation 1.9 %1.9 %Immersion; ISO 62
Melt Flow 9.477 g/10 min
@Load 3.80 kg,
Temperature 230 °C
9.477 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.0 MPa7980 psi50 mm/min; ISO 527
Elongation at Break 25 %25 %ISO 527
Elongation at Yield 4.5 %4.5 %50 mm/min; ISO 527
Tensile Modulus 2.50 GPa363 ksi1 mm/min; ISO 527
Charpy Impact Unnotched 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C
@Temperature 0.000 - 50.0 °C
50.0 µin/in-°F
@Temperature 32.0 - 122 °F
ASTM E831
Vicat Softening Point 96.0 °C205 °FB50; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 707
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.491.49ISO 489
Transmission, Visible 92 %92 %Transmission Factor; DIN 5036
 
Processing PropertiesMetricEnglishComments
Processing Temperature 220 - 260 °C428 - 500 °FBarrel Temperature
Melt Temperature 220 - 260 °C428 - 500 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature <= 85.0 °C<= 185 °FPredrying
Dry Time 2 - 3 hour2 - 3 hourDesiccant-type drier
 
Descriptive Properties
Fire RatingB2DIN 4102

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röhm Plexiglas® zk4HC Molding Compound
Röhm Plexiglas® zk4BR Molding Compound
Röhm Plexiglas® zk30 Molding Compound
Röhm Plexiglas® zk20 Molding Compound
Röhm Plexiglas® zk40 Molding Compound

PHUK057 / 47191

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.