MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Advanced Ceramics ACL 2089 Cordierite
Categories: Ceramic; Glass; Glass Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Cordierite glass-ceramic has good thermal shock properties and is suitable for heat resistant components which undergo rapid thermal cycling.

Information provided by Advanced Ceramics Limited (ACL)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³
Water Absorption 15 %15 %Porosity
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 60.0 MPa8700 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 1.60 µm/m-°C
@Temperature 20.0 - 520 °C
0.889 µin/in-°F
@Temperature 68.0 - 968 °F
Thermal Conductivity 2.00 W/m-K13.9 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1100 °C2010 °FNo Load Condition

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Accuratus MACOR Machinable Glass Ceramic
Advanced Ceramics ACL 2088 Zinc Alumino-Silicate
Borosilicate Glass
96% Silica Consolidated Reconstructed Glass
Advanced Ceramics MEXIM C ACL 2091

CADVC05 / 469

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.