MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Escorene™ UL 7521 Ethylene Vinyl Acetate Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product Description: Escorene Ultra UL 7521 is a high flow, 18.5% VA copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, sealants and wax blends

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Adhesives and Sealants
  • Industrial Sealants
  • Hot Melt Adhesives
  • Wax Blends

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.933 g/cc0.0337 lb/in³ExxonMobil method
Vinyl Acetate Content 18.5 %18.5 %ExxonMobil method
Melt Flow 150 g/10 min
@Load 2.16 kg,
Temperature 190 °C
150 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 80
@Time 15.0 sec
80
@Time 0.00417 hour
ASTM D2240
Hardness, Shore D 28
@Time 15.0 sec
28
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 3.45 MPa500 psiASTM D638
Elongation at Break 610 %610 %ASTM D638
Flexural Modulus, 1% Secant 38.6 MPa5600 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 79.4 °C<= 175 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 43.3 °C110 °FASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Escorene™ UL 7511 Ethylene Vinyl Acetate Copolymer
Braskem Evateno® HM 728 EVA Hot Melt Copolymer
ExxonMobil Escorene® UL-7505 EVA Copolymer, Adhesive and Sealant Grade
Lucobit Lucowax® 1700 Polyethylene Wax
Arkema EVATANE® 20-20 Copolymer Ethylene - Vinyl Acetate

PEX99074 / 175310

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.