MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Edgetek® ET3500-5002 BK Acrylonitrile Styrene Acrylate + PC (ASA+PC)
Categories: Polymer; Thermoplastic; ASA Polymer; Polycarbonate (PC)

Material Notes: The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc
@Temperature 23.0 °C
0.0444 lb/in³
@Temperature 73.4 °F
±0.02; ISO 1183
Filler Content 12 %12 %Glass Fiber Reinforcement
Water Absorption 0.15 %0.15 %@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm0.0010 - 0.0020 in/inASTM D955
Melt Flow 17 - 22 g/10 min
@Load 2.16 kg,
Temperature 300 °C
17 - 22 g/10 min
@Load 4.76 lb,
Temperature 572 °F
ISO 1133
Melt Index of Compound 13 - 16 g/10 min
@Load 21.6 kg,
Temperature 300 °C
13 - 16 g/10 min
@Load 47.6 lb,
Temperature 572 °F
cm³/10min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa
@Thickness 4.00 mm,
Temperature 23.0 °C
14500 psi
@Thickness 0.157 in,
Temperature 73.4 °F
Injection Molded; ISO 527-2/50
Elongation at Break 2.2 %
@Thickness 4.00 mm,
Temperature 23.0 °C
2.2 %
@Thickness 0.157 in,
Temperature 73.4 °F
Injection Molded; ISO 527-2/50
Tensile Modulus 5.90 GPa
@Thickness 4.00 mm,
Temperature 23.0 °C
856 ksi
@Thickness 0.157 in,
Temperature 73.4 °F
Injection Molded; ISO 527-2/1
Charpy Impact Unnotched 3.70 J/cm²
@Temperature 23.0 °C
17.6 ft-lb/in²
@Temperature 73.4 °F
Injection Molded; ISO 179
Charpy Impact, Notched 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
Injection Molded; ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmASTM D257
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HBHBUL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 320 °C536 - 608 °F
Mold Temperature 82.0 - 110 °C180 - 230 °F
Drying Temperature 120 °C248 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
 
Descriptive Properties
FeaturesLow Warpage
FormsPellets
Generic MaterialASA+PC
Generic NameAcrylonitrile Styrene Acrylate + PC (ASA+PC)
Regional AvailabilityEurope
RoHS ComplianceRoHS Compliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Edgetek® ET3500-5001 colored Acrylonitrile Styrene Acrylate + PC (ASA+PC)
DuPont Fusabond® EB560D Ethylene Acrylate Terpolymer
BASF Butyl Acrylate
Arkema LOTRYL® 15 MA 03 Copolymer Ethylene - Methyl Acrylate
Covestro Bayblend® FR 3311 TV PC/ABS Blend, 15% Glass Reinforced

PH0POL1401 / 145970

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.