MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 156 HF Polypropylene (PP), Copolymer - High Flow - Flame Retardant - UL94 V-0  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes:

Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.26 g/cc1.26 g/ccASTM D 792
Water Absorption 0.030 %0.030 %24 hrs @ 23°C; ASTM D 570
Linear Mold Shrinkage 0.012 - 0.017 cm/cm
@Thickness 3.17 mm
0.012 - 0.017 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow 14 - 16 g/10 min
@Load 2.16 kg,
Temperature 230 °C
14 - 16 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 15.9 MPa2300 psiASTM D 638
Elongation at Break >= 200 %>= 200 %ASTM D 638
Tensile Modulus 1.65 GPa240 ksiASTM D 638
Flexural Strength 29.0 MPa4200 psiASTM D 790
Flexural Modulus 1.24 GPa180 ksiASTM D 790
Izod Impact, Notched 0.641 J/cm
@Thickness 3.17 mm
1.20 ft-lb/in
@Thickness 0.125 in
D 256
Izod Impact, Unnotched NB
@Thickness 3.17 mm
NB
@Thickness 0.125 in
ASTM D4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmASTM D 257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 191 - 232 °C375 - 450 °F
Mold Temperature 32.2 - 65.6 °C90.0 - 150 °F
Drying Temperature 79.4 °C175 °F
Dry Time 2 hour2 hour
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 105 CC FR UV Polypropylene (PP), Glass Fiber - Chemically Coupled - Flame Retardant - UV Stabilized
RTP Company RTP 151 HF Polypropylene (PP), High Flow - Flame Retardant - Halogen Free
RTP Company RTP 154 LF Polypropylene (PP), Low Flow - Flame Retardant
RTP Company RTP 154 HI UV Polypropylene (PP), Copolymer - Flame Retardant - UV Stabilized
RTP Company RTP 154 HI Polypropylene (PP), Copolymer - Flame Retardant

PQZWA860 / 92410

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.