MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion Beryllium Copper Alloy 25 Strip; 1/4 H (TD01) Temper (UNS C17200)
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Treatment required for max strength: as supplied
Formability Ratio, 90° Bend, Radius/Thickness (Good Way): 0
Formability Ratio (bad Way): 0
Superficial Hardness: 30T 62-75

Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Key Words: ASTM B-194, QQ-C-533
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.36 g/cc0.302 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 68 - 9068 - 90
Hardness, Vickers 121 - 185121 - 185
Tensile Strength, Ultimate 510 - 610 MPa74000 - 88500 psi
Tensile Strength, Yield 410 - 560 MPa59500 - 81200 psi
Elongation at Break 20 - 45 %20 - 45 %
Modulus of Elasticity 131 GPa19000 ksi
Fatigue Strength 210 - 240 MPa
@# of Cycles 1.00e+8
30500 - 34800 psi
@# of Cycles 1.00e+8
Reverse Bending (R=1)
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000910 - 0.0000115 ohm-cm0.00000910 - 0.0000115 ohm-cm15-19% IACS Conductivity
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 200 °C
9.44 µin/in-°F
@Temperature 68.0 - 392 °F
Thermal Conductivity 105 W/m-K729 BTU-in/hr-ft²-°F
Melting Point 870 - 980 °C1600 - 1800 °F
Solidus 870 °C1600 °F
Liquidus 980 °C1800 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 1.8 - 2.0 %1.8 - 2.0 %
Co + Ni >= 0.20 %>= 0.20 %
Co + Ni + Fe <= 0.60 %<= 0.60 %
Copper, Cu 98 %98 %as balance
Lead, Pb <= 0.020 %<= 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materion Beryllium Copper Alloy 25 Strip; HT (TH04) Temper (UNS C17200)
Beryllium Copper, UNS C17200, TD01 Temper Strip
Materion Beryllium Copper Alloy 3 Strip; HT (TH04) Temper (UNS C17510)
Materion Beryllium Copper Alloy 25 Strip; 1/2H (TD02) Temper (UNS C17200)
Beryllium Copper, UNS C17200, TD02 Temper Strip

NBB580 / 15228

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.