MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 199 X 123298 Polypropylene (PP); High Impact - Permanently Static Dissipative - ESD Protection - UV Stabilized
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: This compound has been formulated to meet the static dissipative requirements of the ATEX Directive.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccASTM D 792
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
@Thickness 3.20 mm
0.010 - 0.020 in/in
@Thickness 0.126 in
ASTM D 955
Melt Flow 8.0 - 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 - 10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 17.2 MPa2500 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Tensile Modulus 0.965 GPa140 ksiASTM D 638
Flexural Strength 24.1 MPa3500 psiASTM D 790
Flexural Modulus 0.827 GPa120 ksiASTM D 790
Izod Impact, Notched 8.01 J/cm
@Thickness 3.20 mm
15.0 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
NB
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Surface Resistance <= 1.00e+9 ohm<= 1.00e+9 ohmESD STM11.11
Static Decay <= 0.50 sec<= 0.50 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 171 - 204 °C340 - 400 °F
Mold Temperature 32.2 - 65.6 °C90.0 - 150 °F
Drying Temperature 79.4 °C
@Time 7200 sec
175 °F
@Time 2.00 hour
Injection Pressure 48.3 - 75.8 MPa7000 - 11000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 199 X 125315 Polypropylene (PP); Permanently Anti-static - ESD Protection
Overview of materials for Polypropylene with 20% Glass Fiber Filler
RTP Company RTP 199 X 110246 D Polypropylene (PP); ESD Protection - Permanently Anti-static
Avient Versalloy™ HC 9210-55N Thermoplastic Elastomer (TPE)
RTP Company RTP 199 X 138766 Z EG Polypropylene (PP); Permanently Static Dissipative - ESD Protection - FDA Compliant Ingredients - Extrusion Grade

PQZRA17663 / 206113

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.