MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eagle Brass 194 HSM® Copper, Hard
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and plateability. Applications include connectors, semiconductor pins and leadframes, sockets and mass terminations.

Information provided by Eagle Brass Company

Key Words: UNS C19400, ASTM B465
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.91 g/cc0.322 lb/in³Annealed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell 30T 61 - 6861 - 68Thickness > 0.020 Inch
Tensile Strength, Ultimate 414 - 483 MPa60000 - 70000 psi
Tensile Strength, Yield 365 - 469 MPa53000 - 68000 psi0.2% offset
Elongation at Break 3.0 - 11 %3.0 - 11 %in 2 in.
Tensile Modulus 121 GPa17500 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000198 ohm-cm0.00000198 ohm-cmAnnealed
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.80 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 259 W/m-K1800 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 97.5 %97.5 %
Iron, Fe 2.35 %2.35 %
Phosphorus, P 0.030 %0.030 %
Zinc, Zn 0.12 %0.12 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eagle Brass 194 HSM® Copper, Extra Hard
Eagle Brass 194 HSM® Copper, 1/2 Hard
Eagle Brass 194 HSM® Copper, Annealed
Eagle Brass 194 HSM® Copper, Extra Spring
Eagle Brass 194 HSM® Copper, Spring

NEAGLE061 / 147310

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.