MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem Green PE SGF4950HS Blow Molded High Density Polyethylene
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Description: SGF4950HS is a High Density Polyethylene, copolymer, offering an outstanding combination of good processability and excellent stress cracking resistance (ESCR). It is recommended for the production of containers, flasks and bottles up to 30 liters for the transport of chemical products. The minimum biobased content of this grade is 95%, determined according to ASTM D6866.

Application: Suggested uses include: Canisters from 2 to 20L for chemical products; Flasks for concentrated detergent. Others applications: Reservoir for wind shield wiper and air ducts.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.951 g/cc0.0344 lb/in³ASTM D792
ESCR 100% Igepal® 1000 hour
@Temperature 50.0 °C
1000 hour
@Temperature 122 °F
F50, molded 2 mm, 0.3 mm notched-plaques; ASTM D1693
ESCR 10% Igepal® 150 hour
@Temperature 50.0 °C
150 hour
@Temperature 122 °F
F50, molded 2 mm, 0.3 mm notched-plaques; ASTM D1693
Melt Flow  0.21 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.21 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 20 g/10 min
@Load 21.6 kg,
Temperature 190 °C
20 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 35.0 MPa5080 psiASTM D638
Flexural Modulus, 1% Secant 1100 MPa160000 psiASTM D790
Izod Impact, Notched 1.75 J/cm3.28 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Feed Temperature 180 °C356 °F
Rear Barrel Temperature 190 °C374 °F
Middle Barrel Temperature 185 °C365 °F
Front Barrel Temperature 180 °C356 °F
Die Temperature 185 °C365 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem Green PE SGD4960 Blow Molded High Density Polyethylene
Braskem Green PE SHE150 Blown Film Extrusion and Cast Film Extrusion High Density Polyethylene
Borealis Borecene™ RM7402 Linear Polyethylene for Rotational Molding
Braskem Green PE SHE150 High Density Polyethylene
Borealis Borecene™ RM7403 Linear Polyethylene for Rotational Molding

PBRASK2004 / 199886

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.