MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil HDP8760.29 Rotational Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Rotational Molding Grade

Material Notes: Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum balance of stiffness, processability and surface appearance.

Availability: Latin America, North America and South America

Additive:

  • Long Term UV-15 Stabilizer: Yes
Applications:
  • Consumer Articles
  • RV tanks
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.948 g/cc0.0342 lb/in³ASTM D4883
ESCR 100% Igepal® 10 hour10 hourASTM D1693 Condition A
ESCR 10% Igepal® 8.0 hour8.0 hourASTM D1693 Condition A
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 23.4 MPa3400 psi2.0 in/min; ASTM D638
Elongation at Yield 20 %20 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1030 MPa150000 psiASTM D790
Impact Test  78.6 J
@Thickness 3.17 mm,
Temperature -40.0 °C
58.0 ft-lb
@Thickness 0.125 in,
Temperature -40.0 °F
ARM
 176 J
@Thickness 6.35 mm,
Temperature -40.0 °C
130 ft-lb
@Thickness 0.250 in,
Temperature -40.0 °F
ARM
 
Thermal PropertiesMetricEnglishComments
Melting Point 131 °C268 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °C165 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 43.0 °C109 °FASTM D648
 
Descriptive Properties
FeaturesLong Term UV 8 Stabilization
Form35 US Mesh Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ICO Polymers ICORENE™ 150-1501 HDPE Rotational Molding Resin
ICO Polymers ICORENE™ 150-1498 HDPE Rotational Molding Resin
A. Schulman SCHULINK® X XL350 Cross-Linkable, High Density Polyethylene
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene
ExxonMobil Paxon™ 7204 Crosslinkable Rotational Molding Resin

PEXB080 / 37385

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.