MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem INSPIRE™ 114 Performance Polypropylene Polymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Blow Molding Grade; Polypropylene, Extrusion Grade; Polypropylene, Impact Modified; Molded/Extruded; Polypropylene, Sheet/Thermoforming Grade

Material Notes:
    Overview
  • High melt strength
  • High toughness
  • Excellent processability
  • High impact and puncture resistance
  • High film stiffness/machinability
  • High heat resistance
  • Complies with U.S. FDA FCN 843, Europe EU-Directive 2002/72/EC

INSPIRE™ 144 Performance Polymer is intended for use in blown film extrusion. Film produced from this resin offers improved stiffness, heat resistance, creep resistance, puncture strength and toughness over competitive polyethylene films. Coextruded structures offer a broad range of potential properties including high stiffness, high clarity, excellent sealability and good barrier properties. INSPIRE 114 Performance Polymer offers high output rates, thin or thick film production with excellent bubble stability, and good gauge uniformity.

INSPIRE™ 114 Performance Polymer is a propylene-based resin that is also intended for use in sheet extrusion, thermoforming, and blow molding.

This product line was spun off from Dow Chemical to Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Thickness 50.8 microns2.00 milFilm Thickness
Melt Index of Compound 0.50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 30.8 MPa4470 psi50.8 microns, Blown Film; ASTM D882
Film Tensile Strength at Yield, TD 25.2 MPa3650 psi50.8 microns, Blown Film; ASTM D882
Tensile Strength, Yield 30.0 MPa4350 psiASTM D638
Film Elongation at Break, MD 700 %700 %50.8 microns, Blown Film; ASTM D882
Film Elongation at Break, TD 850 %850 %50.8 microns, Blown Film; ASTM D882
Film Elongation at Yield, MD 14 %14 %50.8 microns, Blown Film; ASTM D882
Film Elongation at Yield, TD 12 %12 %50.8 microns, Blown Film; ASTM D882
Elongation at Yield 12 %12 %ASTM D638
Flexural Modulus, 1% Secant 1480 MPa215000 psiASTM D790A
Secant Modulus, MD 0.896 GPa130 ksi2% secant modulus; ASTM D882
Secant Modulus, TD 0.772 GPa112 ksi2% secant modulus; ASTM D882
Izod Impact, Notched NBNBASTM D256A
Dart Drop Test 120 g0.265 lb50.8 microns, Blown Film; ASTM D1709A
Film Tensile Strength at Break, MD 47.9 MPa6950 psi50.8 microns, Blown Film; ASTM D882
Film Tensile Strength at Break, TD 36.9 MPa5350 psi50.8 microns, Blown Film; ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 164 °C327 °FDSC; Dow Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Daploy™ WB260HMS Polypropylene
Braskem GF4950HS HDPE Blow Molding Polyethylene Copolymer
Braskem INSPIRE™ 216 Polypropylene Homopolymer
Braskem INSPIRE™ 404 Performance Polypropylene Polymer
Braskem INSPIRE™ 136 Performance Polypropylene Polymer

PDOW0994 / 93330

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.