MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lehvoss LUVOCOM® 1301-9126 PPS, linear with carbon fiber, PTFE, lubricant modified
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler

Material Notes: Properties/attributes include: High continuous-use and heat-distortion temperatures. Non flammable. High-strength and stiffness parts with low creep. Electrically conductive, suitable for continuous discharging of statically-generated electricity. Suitable for metal inserts.

Automotive industry, textile-and office machinery, medical- and precision engineering. Typical uses include: Improved friction and wear behavior. Emergency (dry) running property.

Processing: The material does not necessarily have to be predried; when originally sealed containers are used, this process may normally be omitted. Processing temperatures above 360°C may very rapidly cause thermal damage and should therefore be avoided. Post-crystallization may lead to warpage at elevated operating temperatures. This can be counteracted by suitable heat treatment. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application. High-temperature polymers place increased demands on the tool steels employed.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.49 g/cc1.49 g/ccISO 1183
Moisture Absorption <= 0.0500 %
@Temperature 23.0 °C,
Time 86400 sec
<= 0.0500 %
@Temperature 73.4 °F,
Time 24.0 hour
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inDIN 16901
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 86.0 MPa12500 psiISO 527-2
Elongation at Break 1.3 %1.3 %ISO 527-2
Modulus of Elasticity 10.0 GPa1450 ksiISO 527-2
Flexural Strength 128 MPa18600 psiISO 178
Flexural Modulus 9.00 GPa1310 ksiISO 178
Flexural Strain at Break 1.6 %1.6 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1fu
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 1.00e+6 ohm-cm<= 1.00e+6 ohm-cmIEC 60167
Surface Resistance <= 1e+05<= 1e+05IEC 60093
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 220 °C428 °FContinuous; UL 746B
 240 °C464 °FShort Term
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °FISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 320 - 340 °C608 - 644 °F
Zone 1 300 - 320 °C572 - 608 °F
Zone 2 310 - 330 °C590 - 626 °F
Zone 3 320 - 340 °C608 - 644 °F
Melt Temperature 330 °C626 °F
Mold Temperature 150 - 180 °C302 - 356 °F
Drying Temperature  50.0 - 90.0 °C
@Time >=14400 sec
122 - 194 °F
@Time >=4.00 hour
 100 - 140 °C
@Time 7200 - 14400 sec
212 - 284 °F
@Time 2.00 - 4.00 hour
Dehumidifying dryer
 
Descriptive Properties
Colordark grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lehvoss LUVOCOM® 1301-0915 PPS, linear with carbon fiber, PTFE, lubricant modified
Lehvoss LUVOCOM® 1301-7449 PPS, linear with carbon fiber and PTFE
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
RTP Company RTP 1382 AR 10 TFE 15 Polyphenylene Sulfide (PPS) Carbon Fiber - Aramid Fiber - PTFE Lubricated
RTP Company RTP 1403 P TFE 10 Polyphenyl Sulfone (PPSU), Glass Fiber - PTFE Lubricated - Preliminary Data

PLUU8880 / 193839

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.