MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Overview of materials for Epoxy Adhesive, Flexible
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive, Flexible

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive, Flexible". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Master Bond is a leading manufacturer of high performance epoxy adhesives, sealants, coatings, potting/encapsulation compounds and impregnation resins. Our epoxies include one and two part formulations that can be cured at room temperature, with heat or exposure to UV light. Special formulations feature high electrical and/or thermal conductivity and wide service temperature ranges. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.910 - 3.50 g/cc0.0329 - 0.126 lb/in³Average value: 1.56 g/cc Grade Count:8
Water Absorption 0.500 - 12.2 %0.500 - 12.2 %Average value: 4.47 % Grade Count:18
Viscosity 550 - 350000 cP550 - 350000 cPAverage value: 27500 cP Grade Count:27
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 21.0 - 94.021.0 - 94.0Average value: 56.4 Grade Count:5
 11.0 - 98.0
@Temperature 0.000 - 75.0 °C
11.0 - 98.0
@Temperature 32.0 - 167 °F
Average value: 45.6 Grade Count:6
Hardness, Shore D 60.0 - 89.060.0 - 89.0Average value: 78.8 Grade Count:16
 15.0 - 90.0
@Temperature -60.0 - 75.0 °C
15.0 - 90.0
@Temperature -76.0 - 167 °F
Average value: 73.8 Grade Count:14
Tensile Strength, Ultimate 0.172 - 86.6 MPa25.0 - 12600 psiAverage value: 23.9 MPa Grade Count:21
Elongation at Break 3.20 - 190 %3.20 - 190 %Average value: 78.0 % Grade Count:20
Shear Strength 1.45 - 41.9 MPa210 - 6080 psiAverage value: 19.2 MPa Grade Count:20
 0.690 - 36.887 MPa
@Temperature -55.0 - 121 °C
100 - 5350.0 psi
@Temperature -67.0 - 250 °F
Average value: 12.6 MPa Grade Count:20
Adhesive Bond Strength 6.21 - 36.5 MPa900 - 5300 psiAverage value: 24.6 MPa Grade Count:9
 1.37895 - 30.3369 MPa
@Temperature -54.4 - 93.3 °C
200.000 - 4400.01 psi
@Temperature -66.0 - 200 °F
Average value: 16.1 MPa Grade Count:9
Peel Strength 5.26 - 7.01 kN/m30.0 - 40.0 pliAverage value: 6.57 kN/m Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00100 - 4.40e+16 ohm-cm0.00100 - 4.40e+16 ohm-cmAverage value: 1.92e+15 ohm-cm Grade Count:19
 2.90e+7 - 2.50e+13 ohm-cm
@Temperature 100 - 150 °C
2.90e+7 - 2.50e+13 ohm-cm
@Temperature 212 - 302 °F
Average value: 1.03e+12 ohm-cm Grade Count:10
Surface Resistance 5.00 - 40.0 ohm
@Temperature 75.0 - 75.0 °C
5.00 - 40.0 ohm
@Temperature 167 - 167 °F
Average value: 15.0 ohm Grade Count:3
Shielding Effectiveness 40.0 - 110 dB40.0 - 110 dBAverage value: 65.0 dB Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.0 - 73.0 µm/m-°C7.22 - 40.6 µin/in-°FAverage value: 34.8 µm/m-°C Grade Count:6
Thermal Conductivity 0.720 - 2.16 W/m-K5.00 - 15.0 BTU-in/hr-ft²-°FAverage value: 1.47 W/m-K Grade Count:5
Maximum Service Temperature, Air 121 - 204 °C250 - 400 °FAverage value: 149 °C Grade Count:5
Minimum Service Temperature, Air -62.2 - -51.1 °C-80.0 - -60.0 °FAverage value: -60.0 °C Grade Count:5
Glass Transition Temp, Tg 42.0 - 115 °C108 - 239 °FAverage value: 73.8 °C Grade Count:6
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 149 °C68.0 - 300 °FAverage value: 68.7 °C Grade Count:12
Cure Time 480 - 4320 min8.00 - 72.0 hourAverage value: 1360 min Grade Count:6
 23.0 - 120 min
@Temperature 65.6 - 149 °C
0.383 - 2.00 hour
@Temperature 150 - 300 °F
Average value: 76.8 min Grade Count:7
Pot Life 9.00 - 180 min9.00 - 180 minAverage value: 64.2 min Grade Count:28

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Adhesive
Overview of materials for Epoxy/Carbon Fiber Composite
Overview of materials for Thermoset Polyurethane, Adhesive
Overview of materials for Epoxy Cure Resin
Overview of materials for Cyanoacrylate Adhesive

O1771 / 77903

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.