MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Performance Polymers IPS II PPL-C4050 PEKK (Polyetherketoneketone) Linear Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyketone; PEKK, Unreinforced

Material Notes: Amber pellets; neat resin

Information provided by Infinite Polymer System II.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ASTM D792
Water Absorption <= 0.20 %<= 0.20 %24 hr; ASTM D570
Linear Mold Shrinkage 0.010 cm/cm0.010 in/in
Melt Flow 120 g/10 min
@Load 8.40 kg,
Temperature 360 °C
120 g/10 min
@Load 18.5 lb,
Temperature 680 °F
Crystallinity 32 %32 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8888ASTM D785
Tensile Strength at Break 110 MPa16000 psiASTM D638
Elongation at Break >= 12 %>= 12 %ASTM D638
Modulus of Elasticity 4.40 GPa638 ksiASTM D638
Flexural Yield Strength 193 MPa28000 psiASTM D790
Flexural Modulus 4.60 GPa667 ksiASTM D790
Compressive Yield Strength 207 MPa30000 psiASTM D695
Poissons Ratio 0.400.40
Shear Modulus 1.57 GPa228 ksiCalculated
Shear Strength 138 MPa20000 psiASTM D732
Izod Impact, Notched 0.530 J/cm
@Thickness 3.17 mm
0.993 ft-lb/in
@Thickness 0.125 in
ASTM D256
Coefficient of Friction 0.1730.173ASTM D1894
Coefficient of Friction, Static 0.2620.262ASTM D1894
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Surface Resistance 2.00e+16 ohm2.00e+16 ohmASTM D257
Dielectric Constant 3.3
@Frequency 1000 Hz
3.3
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 23.6 kV/mm599 kV/inASTM D149
Dissipation Factor 0.0040
@Frequency 1000 Hz
0.0040
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.0 µm/m-°C11.7 µin/in-°FBelow glass transition temp; ASTM D696
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°FASTM C177
Melting Point 360 °C680 °FDSC
Maximum Service Temperature, Air 260 °C500 °FUL Continuous Use Temp.
Deflection Temperature at 1.8 MPa (264 psi) 175 °C347 °FASTM D648
Glass Transition Temp, Tg 160 °C320 °FDSC
Flammability, UL94 V-0V-0
Smoke Density <= 10<= 10NBS
Oxygen Index 40 %40 %ASTM D2863

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Performance Polymers IPS II PPL-C1050 PEKK (Polyetherketoneketone) Linear Extrusion Grade
Murtfeldt Murpec® Polyetheretherketone
Performance Polymers IPS II PPL-A1050 PEKK (Polyetherketoneketone) Branched Standard Grade
Overview of materials for Polyetherketoneketone (PEKK), Reinforced
Performance Polymers IPS II PPL-C4150 PEKK (Polyetherketoneketone) Linear 30% Glass Fiber Reinforced Molding Grade

PPEKK02 / 56103

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.