MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Latrobe LSS™ A2 Tool Steel (ASTM A2)
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; High Carbon Steel; Tool Steel; Air-Hardening Steel

Material Notes: TLS A2 tool steel is a versatile, air-hardening tool steel that is characterized by good toughness and excellent dimensional stability in heat treatment. TLS A2 is intermediate in wear resistance between O1 oil-hardening tool steel and D2 high-carbon, high-chromium tool steel. TLS A2 provides an effective combination of strength and toughness, tool performance, price, and a wide variety of product forms. Typical applications for TLS A2 tool steel include punches and dies, chuck jaws, cutting tools for woodworking, tooling for plastic injection, dowel pins, hammers, industrial knives, and gages.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.86 g/cc7.86 g/cc
Density 7.86 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 6363Air Cooled from 982°C, 30 minutes
 63.563.5Air Cooled from 1038°C, 30 minutes
 6464Air Cooled from 1010°C, 30 minutes
Modulus of Elasticity 207 GPa30000 ksi
Machinability 70 %70 %1% Carbon Steel
Izod Impact Unnotched 67.8 J50.0 ft-lbAir Cooled from 954°C; 94°C Temper Temperature
 122 J90.0 ft-lbAir Cooled from 954°C; 316°C Temper Temperature
 229 J169 ft-lbAir Cooled from 954°C; 649°C Temper Temperature
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.6 µm/m-°C
@Temperature 93.0 - 260 °C
5.89 µin/in-°F
@Temperature 199 - 500 °F
 14.0 µm/m-°C
@Temperature 93.0 - 649 °C
7.78 µin/in-°F
@Temperature 199 - 1200 °F
Thermal Conductivity 26.001 W/m-K180.44 BTU-in/hr-ft²-°F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 793 °C1460 °FCritical Temperaure Ac1
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.0 %1.0 %
Chromium, Cr 5.0 %5.0 %
Iron, Fe 91.7 %91.7 %
Manganese, Mn 0.75 %0.75 %
Molybdenum, Mo 1.0 %1.0 %
Silicon, Si 0.30 %0.30 %
Vanadium, V 0.25 %0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type A2 Tool Steel
Bohler-Uddeholm AISI A2 Cold Work Tool Steel
Carpenter No. 484® (Carpenter Air-Hard; AISI A2)
Crucible Steel AIRKOOL® (AISI A2) Tool Steel
ATI Allegheny Ludlum A2 Tool Steel, UNS T30102

NTIMK099 / 19446

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.