MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay MACKADET® EQ-112 Surfactant  (discontinued **)
Categories: Fluid

Material Notes: Product Description: Mackadet EQ-112 is mild blend of ingredients for the formulation of tear-free baby shampoos. Dilution at 27% in water gives a standard baby shampoo.

Uses: Foam Pump, Bubble Baths, Facial/Body Wash, Baby/Kid Shampoos.

Note: Tear free claims require tests to be performed by the customer using fragrance, dyes and preservatives etc. The ingredients of Mackadet EQ-112 make favorable results probable.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.058 g/cc0.03822 lb/in³
Solids Content >= 41 %>= 41 %Moisture Balance
pH 6.3 - 7.36.3 - 7.3
Viscosity <= 6000 cP<= 6000 cP#3 SP @ 12 rpm
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 4.0<= 4.0
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceClear Liquid
CompositionA. NigerAbsent
 Candida AlbicansAbsent
 Gram Negative BacteriaAbsent
 Staphylococcus AureusAbsent
 Total Plate Count<500 cfu/g
 Yeast and Molds<10
PreservativeQuaternium0.001

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay MACKADET® DR-100M Surfactant
Solvay MACKADET® SBC--8 Surfactant
Solvay MACKADET® EQ-178 Surfactant
Solvay MACKADET® CA-ND Surfactant
Verdant Specialty Solutions MACKADET® 40-K Surfactant

WRHOD190 / 137421

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.