MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Niagara LaSalle StressProof® Cold Finished Steel Bar
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel

Material Notes: StressProof® is made by a patented process which consists of drawing the bar through a special die under heavy draft, then stress relieving it in a precisely controlled furnace. StressProof® offers wearability without case hardening, strength without heat treating, plus excellent machinability and tool life. Other benefits include resistance to fatigue and stress, balanced working, and minimum warpage and distortion. StressProof® can also be induction hardened but should be watched for quench cracks, and, being a resulfurized steel, a magnetic particle inspection operation should be performed after heat treating.

Information provided by Niagra LaSalle Corporation

Key Words: AISI 1144; ASTM A311
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 793 MPa>= 115000 psi
Tensile Strength, Yield >= 689 MPa>= 100000 psi
Elongation at Break >= 8.0 %>= 8.0 %7% min above 3 in
Reduction of Area >= 25 %>= 25 %20% min above 2
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.40 - 0.48 %0.40 - 0.48 %
Iron, Fe 97.15 - 97.86 %97.15 - 97.86 %as balance
Manganese, Mn 1.35 - 1.65 %1.35 - 1.65 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si 0.15 - 0.35 %0.15 - 0.35 %
Sulfur, S 0.24 - 0.33 %0.24 - 0.33 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Niagara LaSalle Fatigue-Proof® Cold Finished Steel Bar
AISI 4140 Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round
AISI 1018 Steel, as cold drawn, 22-32 mm (0.875-1.25 in) round
AISI 1144 Steel, cold drawn, low temperature, stress relieved, 22-32 mm (0.875-1.25 in) round
AISI 1144 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round

NNIAL001 / 160291

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.